Mould-proof preservative treatment technology for furniture
A technology for anti-corrosion treatment and furniture. It is used in pretreatment surfaces, paints containing biocides, and antifouling/underwater coatings. The effect of anti-fungal performance, long-term safety performance and excellent appearance performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] The anti-mildew and anti-corrosion treatment process for furniture of the present invention comprises the following steps: 1) cutting, planing, bonding and assembling the wood into complete furniture; 2) putting the furniture into a vacuum drying box for drying treatment, vacuum drying The temperature is 80kpa, the temperature is 50°C, and it lasts for 40 minutes; 3) Spray the topcoat with anti-mildew and anti-corrosion function on the furniture surface dried in step 2), put it into the heating box after drying at room temperature, and apply pressure to the air in the heating box 1.0Mpa, the temperature is 70°C, and steam is introduced at the same time, and the steam flow rate is 0.7m 3 / h, after 2 hours of treatment, stop steaming and lower the temperature to 50°C to dry for 20 minutes; 4) Repeat and evenly spray the topcoat on the furniture in step 3), and put it into the heating box after drying at room temperature. The pressure of the internal air is 2.0Mpa, the tem...
Embodiment 2
[0019] The anti-mildew and anti-corrosion treatment process for furniture of the present invention comprises the following steps: 1) cutting, planing, bonding and assembling the wood into complete furniture; 2) putting the furniture into a vacuum drying box for drying treatment, vacuum drying The temperature is 95kpa, the temperature is 55°C, and lasts for 50 minutes; 3) Spray the surface of the furniture after drying in step 2) with a topcoat with anti-mildew and anti-corrosion functions, dry it at room temperature, put it into the heating box, and apply pressure to the air in the heating box 1.5Mpa, the temperature is 75°C, and steam is introduced at the same time, and the steam flow rate is 0.9m 3 / h, after 3 hours of treatment, stop steaming and lower the temperature to 55°C to dry for 30 minutes; 4) Repeat and evenly spray the topcoat on the furniture in step 3), and put it into the heating box after drying at room temperature. The pressure of the internal air is 2.5Mpa, ...
Embodiment 3
[0022]The anti-mildew and anti-corrosion treatment process for furniture of the present invention comprises the following steps: 1) cutting, planing, bonding and assembling the wood into complete furniture; 2) putting the furniture into a vacuum drying box for drying treatment, vacuum drying The temperature is 90kpa, the temperature is 53°C, and lasts for 45 minutes; 3) Spray the surface of the furniture after drying in step 2) with a topcoat with anti-mildew and anti-corrosion functions, and put it into the heating box after drying at room temperature, and apply pressure to the air in the heating box 1.3Mpa, temperature 73°C, steam is introduced at the same time, the steam flow rate is 0.8m 3 / h, after 3 hours of treatment, stop steaming and lower the temperature to 55°C to dry for 25 minutes; 4) Repeat and evenly spray the topcoat on the furniture in step 3), and put it into the heating box after drying at room temperature. The pressure of the internal air is 2.5Mpa, the tem...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com