Processing technology of soft fading-prevention denim
A processing technology and anti-fading technology, applied in the field of textile fabrics, to achieve the effects of high degree of automation, comfortable wearing and simple preparation process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] A kind of processing technology of soft anti-fading denim, its preparation process is:
[0015] 1) The preparation process of nano-silver oxide is: mix sucrose ester, silver nitrate and 1.4% NaOH aqueous solution in a mass ratio of 6 / 11 / 100, react at 36°C for 50min, place for 20h, and centrifuge at 3800r / min, the product Wash with absolute ethanol and distilled water three times in sequence, and dry the washed product in a vacuum oven at 60°C for 1 day to obtain nano-silver oxide;
[0016] 2) The preparation process of the modified polyester fiber is as follows: mix nano-silver oxide with polyester chips, the mass ratio of nano-silver oxide and polyester chips in the mixture is 0.2 / 100, and then add active polypeptide accounting for 0.1% of the mass of polyester chips , melted at 265°C, and then extruded from the spinneret hole of the spinneret at 265°C, cooled and solidified into filaments in water to obtain a modified polyester fiber, wherein the amino acid sequence o...
Embodiment 2
[0020] A kind of processing technology of soft anti-fading denim, its preparation process is: at first, the preparation process of nano-silver oxide is: sucrose ester, silver nitrate and 1.6% NaOH aqueous solution are mixed according to mass ratio 8 / 14 / 100, in 39 React at ℃ for 60 minutes, place it for 24 hours, centrifuge at 4000r / min, wash the product three times with absolute ethanol and distilled water in turn, and dry the washed product in a vacuum oven at 60℃ for 1 day to obtain nano-silver oxide; The preparation process of the modified polyester fiber is as follows: mix nano-silver oxide with polyester chips, the mass ratio of nano-silver oxide and polyester chips in the mixture is 0.5 / 100, then add active polypeptide accounting for 0.2% of the weight of polyester chips, Melt at 275°C, then extrude the melt from the spinneret hole at 275°C, cool and solidify in water to form filaments, and obtain modified polyester fibers, in which the amino acid sequence of the active p...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com