Embodiment 1
[0049] An anti-drop eye shadow block, which comprises the following components in parts by weight:
[0050] 50 parts of talcum powder,
[0052] 5 parts kaolin,
[0053] 20 servings of pearl powder,
[0054] 5 parts of acetylated lanolin alcohol,
[0055] 8 parts of zinc stearate,
[0056] Tween-20 5 parts,
[0057] 3 parts of ethyl citronellyl oxalate mixed ester,
[0058] 3 parts of pearlescent pigment,
[0059] 5 parts of water.
[0060] The specific preparation method is:
[0061] (1) Dry talc powder, zinc oxide, kaolin, pearl powder, zinc stearate, and pearlescent pigments and mix them for a single grinding, and then sieving after grinding;
[0062] (2) Then mix the material obtained in step (1) with acetylated lanolin alcohol, ethyl citronellyl oxalate mixed ester, and water, and stir evenly;
[0063] (3) Perform secondary grinding of the mixture obtained in step (2) to ensure that the particle diameter of the mixture after grinding is 150 nm;
[0064] (4) The ...
Embodiment 2
[0066] An anti-drop eye shadow block, which comprises the following components in parts by weight:
[0067] 50 parts of talcum powder,
[0068] 1 part of zinc oxide,
[0069] 5 parts kaolin,
[0070] 20 servings of pearl powder,
[0071] 3 parts of acetylated lanolin alcohol,
[0072] 8 parts of zinc stearate,
[0073] Tween-20 5 parts,
[0074] 8 parts of water.
[0075] The specific preparation method is:
[0076] (1) Dry talc powder, zinc oxide, kaolin, pearl powder, zinc stearate, and pearlescent pigments and mix them for a single grinding, and then sieving after grinding;
[0077] (2) Then mix the material obtained in step (1) with acetylated lanolin alcohol, ethyl citronellyl oxalate mixed ester, and water, and stir evenly;
[0078] (3) Perform secondary grinding of the mixture obtained in step (2) to ensure that the particle size of the mixture after grinding is 200 nm;
[0079] (4) The mixture obtained in step (3) is compressed by a powder press to form an eye shadow block.
Embodiment 3
[0081] An anti-drop eye shadow block, which comprises the following components in parts by weight:
[0082] 30 parts of talcum powder,
[0083] 3 parts of zinc oxide,
[0084] 5 parts kaolin,
[0085] 25 parts of pearl powder,
[0086] 5 parts of acetylated lanolin alcohol,
[0087] 12 parts of zinc stearate,
[0088] Tween-20 10 parts,
[0089] 10 parts of water.
[0090] The specific preparation method is:
[0091] (1) Dry talc powder, zinc oxide, kaolin, pearl powder, zinc stearate, and pearlescent pigments and mix them for a single grinding, and then sieving after grinding;
[0092] (2) Then mix the material obtained in step (1) with acetylated lanolin alcohol, ethyl citronellyl oxalate mixed ester, and water, and stir evenly;
[0093] (3) Perform secondary grinding of the mixture obtained in step (2) to ensure that the particle size of the mixture after grinding is 100 nm;
[0094] (4) The mixture obtained in step (3) is compressed by a powder press to form an eye shadow block.
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com