Problems solved by technology

[0003] Wood, boards, furniture, walls and other paints in the family room will contain formaldehyde, but what is even more frightening is that the release period of formaldehyde is generally three to fifteen years, resulting in the slow release of formaldehyde into the air to pollute the environment

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0015] A water-based paint for interior decoration, which consists of the following components in parts by weight: 210 parts of styrene-acrylic polymer emulsions, 35 parts of water-based alkyd resins, 55 parts of aminopropylamine dioleate, 90 parts of diatomaceous earth, calcite 40 parts of powder, 25 parts of talc, 10 parts of polyacrylate, 15 parts of propylene glycol butyl ether, 5 parts of hydroxyethyl cellulose, 7 parts of tributyl phosphate and 250 parts of water.

[0016] A preparation method of water-based paint for interior decoration, comprising the following steps:

[0017] (1) Put styrene-acrylic polymer emulsion, water-based alkyd resin, aminopropylamine dioleic acid, polyacrylate, propylene glycol butyl ether, hydroxyethyl cellulose and tributyl phosphate into the dispersion container according to the formula, and stir while feeding. , control the rotation speed to 800 rpm, and stir for 15 minutes to obtain a uniform mixed solution system;

[0018] (2) Then add ...

Embodiment 2

[0020] A water-based paint for interior decoration, which is made up of the following components in parts by weight: 200 parts of styrene-acrylic polymer emulsions, 40 parts of water-based alkyd resins, 50 parts of aminopropylamine dioleate, 100 parts of diatomaceous earth, calcite 30 parts of powder, 30 parts of talc, 5 parts of polyacrylate, 20 parts of propylene glycol butyl ether, 3 parts of hydroxyethyl cellulose, 10 parts of tributyl phosphate and 240 parts of water.

[0021] A preparation method of water-based paint for interior decoration, comprising the following steps:

[0022] (1) Put styrene-acrylic polymer emulsion, water-based alkyd resin, aminopropylamine dioleic acid, polyacrylate, propylene glycol butyl ether, hydroxyethyl cellulose and tributyl phosphate into the dispersion container according to the formula, and stir while feeding. , control the rotation speed to 800 rpm, and stir for 20 minutes to obtain a uniform mixed solution system;

[0023] (2) Then a...

Embodiment 3

[0025] A water-based paint for interior decoration, which is made up of the following components in parts by weight: 220 parts of styrene-acrylic polymer emulsions, 30 parts of water-based alkyd resins, 60 parts of aminopropylamine dioleate, 80 parts of diatomaceous earth, calcite 50 parts of powder, 20 parts of talc, 15 parts of polyacrylate, 10 parts of propylene glycol butyl ether, 8 parts of hydroxyethyl cellulose, 5 parts of tributyl phosphate and 260 parts of water.

[0026] A preparation method of water-based paint for interior decoration, comprising the following steps:

[0027] (1) Put styrene-acrylic polymer emulsion, water-based alkyd resin, aminopropylamine dioleic acid, polyacrylate, propylene glycol butyl ether, hydroxyethyl cellulose and tributyl phosphate into the dispersing container according to the formula, and stir while feeding. , control the rotating speed to 800 rpm, and stir for 25 minutes to obtain a uniform mixed solution system;

[0028] (2) Then ad...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a waterborne coating for indoor decoration. The waterborne coating for indoor decoration is prepared from the following components in parts by weight: 200-220 parts of a polymerized styrene-acrylic emulsion, 30-40 parts of aqueous alkyd resin, 50-60 parts of aminopropylamine dioleate, 80-100 parts of diatomite, 30-50 parts of calcite in powder, 20-30 parts of talc powder, 5-15 parts of polyacrylate, 10-20 parts of propanediol butyl ether, 3-8 parts of hydroxyethyl cellulose, 5-10 parts of tributyl phosphate and 240-260 part of water. The waterborne coating for indoor decoration is environment-friendly and non-toxic, and ensures health of body of people. The cured coating is extremely high in hardness and extremely good in tear resistance. The coating solves the problem that the coating on a wall is cracked and falls off as the base layer of the wall is not firm, and can be widely applied to the field of decoration.

Description

technical field [0001] The invention belongs to the technical field of coatings, in particular to a water-based paint for interior decoration and a preparation method. Background technique [0002] Many indoor decoration coatings contain formaldehyde and other harmful substances, among which formaldehyde is a carcinogenic and teratogenic substance. Formaldehyde is a recognized source of allergy and one of the potential strong mutagens, and it is also one of the risk factors for childhood leukemia. According to domestic medical journals and related literature reports, the harm of indoor formaldehyde to human health can be summarized as irritant, toxic and carcinogenic. [0003] The wood, planks, furniture, walls and other coatings in the family room will contain formaldehyde. However, what is even more frightening is that the release period of formaldehyde is generally three to fifteen years, resulting in the slow release of formaldehyde into the air to pollute the environme...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D125/14C09D167/08C09D7/61C09D7/63
CPCC08L2205/035C09D7/61C09D7/63C09D7/70C09D125/14C08L67/08C08L33/04C08L1/284C08K13/04C08K7/26C08K3/34C08K5/06C08K5/521
Inventor 梁柳艳刘德烽
Owner 柳州市家富连装饰有限公司