A method of using magnetic hydrophobic particles to strengthen the flotation of refractory nickel sulfide ore
A technology of hydrophobic particles and nickel sulfide ore, applied in flotation, solid separation and other directions, can solve the problems of difficult to improve recovery rate, small particle size of fine-grained nickel sulfide ore, easy to oxidize, etc., to achieve low cost and enhanced surface hydrophobicity. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] Grind a nickel sulfide ore to -0.074mm, accounting for 80%, add 400g / t dispersant sodium hexametaphosphate, 300g / t inhibitor yellow potato gum, 100g / t collector butyl xanthate and 20g / t t The foaming agent MIBC is used for stirring and slurry mixing and roughing of nickel sulfide minerals to obtain roughing concentrates and roughing tailings. Add the collector butyl xanthate and foaming agent MIBC to the obtained roughing tailings and perform two sweeps to obtain the sweeping tailings. The sweeping sequence returns to the upper level operation, and the first sweeping adds 50g / t capture Collector xanthate, 20g / t foaming agent MIBC, add 30g / t collector xanthate, 10g / t foaming agent MIBC in the second sweep. Adding dispersant sodium hexametaphosphate and inhibitor yellow potato gum to the roughing concentrate to carry out three times of beneficiation to obtain concentrate 1, and the selected middle ore will return to the previous operation in sequence. Among them, the firs...
Embodiment 2
[0034] Grind a nickel sulfide ore to -0.074mm, accounting for 85%, add 500g / t dispersant sodium hexametaphosphate, 200g / t inhibitor yellow potato gum, 80g / t collector butyl xanthate and 20g / t t The foaming agent MIBC is used for stirring and slurry mixing and roughing of nickel sulfide minerals to obtain roughing concentrates and roughing tailings. Add the collector butyl xanthate and the foaming agent MIBC to the obtained roughing tailings, and perform two sweeps to obtain the sweeping tailings. The sweeping sequence returns to the upper level operation, and the first sweeping adds 40g / t trapping Collector xanthate, 20g / t foaming agent, add 20g / t collector xanthate, 10g / t foaming agent MIBC in the second sweep. The dispersant sodium hexametaphosphate and inhibitor yellow potato gum are included in the roughing concentrate for three times of beneficiation to obtain concentrate 1, and the selected middle ore will return to the previous operation in sequence. Among them, the fir...