Finished fabric and manufacture process thereof
A finished product and chemical fiber technology, applied in the field of finished cloth and its manufacturing process, can solve the problems of low output of finished cloth production process, and achieve the effects of low average dyeing cost, increased output and reduced production cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] A finished cloth and a manufacturing process thereof, comprising the following steps:
[0025] S1. 30 parts of polymerized chemical fiber POY, 3 parts of polyester, 6 parts of spandex, 6 parts of cotton fiber, 3 parts of acrylic fiber, 5 parts of viscose, 10 parts of polyamide, and 2 parts of calcium carbonate are filtered, measured, and twisted by an elastic machine. DTY chemical fiber yarn is produced by texturing, and there is no special requirement in the production process;
[0026] S2. Use the DTY chemical fiber yarn to produce 305cm gray cloth every day through the water jet machine, the deviation of the warp density shall not exceed -1.5%, and the deviation of the weft density shall not exceed -1.0%;
[0027] S3, place the door-width gray cloth in the dyeing equipment, and put 10 parts of dyeing agent into the dyeing equipment, 4 parts of anti-fading agent, 3 parts of sodium hydroxide, adjust the pH of the dyeing solution to 7.5-8, pretreatment, dyeing Three ho...
Embodiment 2
[0031] A finished cloth and a manufacturing process thereof, comprising the following steps:
[0032] S1. 35 parts of polymerized chemical fiber POY, 4 parts of polyester, 7 parts of spandex, 7 parts of cotton fiber, 4 parts of acrylic fiber, 8 parts of viscose, 15 parts of polyamide, and 3 parts of calcium carbonate are filtered, measured, and twisted by an elastic machine. DTY chemical fiber yarn is produced by texturing, and there is no special requirement in the production process;
[0033] S2. Use the DTY chemical fiber yarn to produce 305cm gray cloth every day through the water jet machine, the deviation of the warp density shall not exceed -1.5%, and the deviation of the weft density shall not exceed -1.0%;
[0034] S3, place the door-width gray cloth in the dyeing equipment, and put 11 parts of dyeing agent into the dyeing equipment, 5 parts of anti-fading agent, 4 parts of sodium hydroxide, adjust the pH of the dyeing solution to 7.5-8, pretreatment, dyeing Three ho...
Embodiment 3
[0038] A finished cloth and a manufacturing process thereof, comprising the following steps:
[0039] S1. Filter and measure 40 parts of polymerized chemical fiber POY, 5 parts of polyester, 8 parts of spandex, 8 parts of cotton fiber, 5 parts of acrylic fiber, 11 parts of viscose, 20 parts of polyamide, and 4 parts of calcium carbonate. DTY chemical fiber yarn is produced by texturing, and there is no special requirement in the production process;
[0040] S2. Use the DTY chemical fiber yarn to produce 305cm gray cloth every day through the water jet machine, the deviation of the warp density shall not exceed -1.5%, and the deviation of the weft density shall not exceed -1.0%;
[0041] S3. Place the door-width gray cloth in the dyeing equipment, and put 12 parts of dyeing agent into the dyeing equipment, 6 parts of anti-fading agent, 5 parts of sodium hydroxide, adjust the pH of the dyeing solution to 7.5-8, pretreatment and dyeing Three hours, water washing, reduction clean...
PUM