A kind of disperse dye ink for thermal transfer printing of thin paper and preparation method thereof
A technology of disperse dyes and thermal transfer printing, applied in transfer printing method, dyeing method, printing and other directions, can solve the problem of high requirements on paper weight, and achieve good printing smooth performance, good fabric feel and good fluency. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Embodiment 1: prepare yellow ink
[0025] 1. Take 40g of disperse dye yellow 54, 14g of acrylic modified resin, 7.5g of acrylic resin, 7.5g of polyethylene glycol 1000, 7.5g of sodium lignosulfonate, and 243ml of deionized water, first use a mixer Stir at a low speed of 200 rpm for 30 minutes, then grind for 3 hours in a grinding and dispersing machine at 5000-10000 rpm to obtain 400 g of pigment paste with a solid content of 10%, requiring the solids (pigment and dispersant) therein The particle size is 100-300nm.
[0026] 2. Add 300ml of deionized water to the pigment paste, and while stirring in a blender (speed 200 rpm), add 240g of glycerin, 15g of humectant mixed in equal volume ratio of diethylene glycol and diethylene glycol ether , Triton X-100 surfactant 5g, after 30 minutes, add pH adjuster monoethanolamine 20g, and add antibacterial agent chlorocresol 10g.
[0027] 3. Filter the mixed ink with a 1um microporous membrane, and then further filter the filtrat...
Embodiment 2
[0029] Embodiment 2: prepare cyan ink
[0030] 1. Take 40g of disperse dye blue 359, 7.5g of acrylic resin, 7.5g of polyethylene glycol 1000, 7.5g of sodium lignosulfonate, and 243ml of deionized water, first use a mixer at a low speed of 200 rpm Stir for 30 minutes, then grind for 3 hours in a grinding and dispersing machine at 5000-10000 rpm to obtain 400 g of pigment paste with a solid content of 10%, and the particle size of the solid (pigment and dispersant) in it is required to be 100-300nm .
[0031] 2. Add 300ml of deionized water to the pigment paste, and while stirring in a blender (speed 200 rpm), add 240g of glycerin, 15g of humectant mixed in equal volume ratio of diethylene glycol and diethylene glycol ether , Triton X-100 surfactant 5g. After 30 minutes, 20 g of the pH regulator monoethanolamine was added, and 10 g of the bacteriostatic agent chlorocresol was added.
[0032] 3. Filter the mixed ink with a 0.8um microporous membrane, and then further filter th...
Embodiment 3
[0034] Example 3: Preparation of magenta ink
[0035] 1. Take 40g of disperse red 60, 7.5g of acrylic resin, 7.5g of polyethylene glycol 1000, 7.5g of sodium lignosulfonate, and 243ml of deionized water, first stir with a mixer at a speed of 200 rpm 30 minutes, then grind for 3 hours in a 5000-10000 rev / min grinding disperser to obtain 400 g of disperse dye color paste with a dye solid content of 10%, requiring the particle size of the solid (pigment and dispersant) to be 100-300nm .
[0036] 2. Add 300ml of deionized water to the pigment paste, and while stirring in a blender (speed 200 rpm), add 240g of glycerin, 15g of humectant mixed in equal volume ratio of diethylene glycol and diethylene glycol ether , Triton X-100 surfactant 5g, after 30 minutes, add pH adjuster monoethanolamine 20g, and add antibacterial agent chlorocresol 10g.
[0037] 3. Filter the mixed ink with a 1.0um microporous membrane, and then further filter the filtrate with a 0.2um microporous membrane t...
PUM
| Property | Measurement | Unit |
|---|---|---|
| viscosity | aaaaa | aaaaa |
| surface tension | aaaaa | aaaaa |
| diameter | aaaaa | aaaaa |