A kind of production method of needle coke

A production method, needle coke technology, applied in coking ovens, tar pitch/petroleum pitch/natural pitch processing, coking carbonaceous materials, etc., can solve problems such as low yield, high cost, unfavorable market competition, etc., to achieve The effect of low cost, increased coking speed, and simple process

Active Publication Date: 2021-05-04
恒源碳材料股份有限公司
View PDF5 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] At present, coal-based needle coke is mainly used in China, but the preparation process of coal-based needle coke of various manufacturers is classified as confidential or protected by patents, and the production cost is relatively high and the yield is low. Conducive to the current fierce market competition

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] A method for producing needle coke, comprising the following steps:

[0017] S1, take out kerosene and anthracene oil according to the ratio of 1:1.6, and mix evenly, make solvent;

[0018] S2. Take out the solvent and soft asphalt according to the ratio of 1:2, mix them evenly, put them into a settling tank for sedimentation, and finally separate the light phase and heavy phase; heat to 140°C during mixing, and then put them in a mixer and stir for 2 hours ;

[0019] S3. Heat the heavy phase obtained in S1 to 180°C, then pump it to the dehydration tower, separate the water in the dehydration tower, introduce it into the tube furnace, heat it to 320°C through the tube furnace, and introduce it into the distillation tower for distillation. The oil gas in the distillation becomes light oil after being cooled by the condensation tower, and the bitumen after distillation is discharged for standby;

[0020] S4. Heating the pitch prepared in S3 to 480° C. and then introduci...

Embodiment 2

[0025] A method for producing needle coke, comprising the following steps:

[0026] S1, take out kerosene and anthracene oil according to the ratio of 1:1.8, and mix evenly, make solvent;

[0027] S2. Take out the solvent and soft asphalt according to the ratio of 1:1.8, mix them evenly, put them into a settling tank for sedimentation, and finally separate the light phase and heavy phase; heat to 120°C when mixing, and then put it in a mixer and stir for 1 hour ;

[0028] S3. Heat the heavy phase obtained in S1 to 160°C, then pump it to the dehydration tower, separate the water in the dehydration tower, introduce it into the tube furnace, heat it to 340°C through the tube furnace, and introduce it into the distillation tower for distillation. The oil gas in the distillation becomes light oil after being cooled by the condensation tower, and the bitumen after distillation is discharged for standby;

[0029] S4. Heating the pitch prepared in S3 to 500° C. and then introducing ...

Embodiment 3

[0034] A method for producing needle coke, comprising the following steps:

[0035] S1, kerosene and anthracene oil are taken out according to the ratio of 1:1.7, and mix uniformly, make solvent;

[0036] S2. Take out the solvent and soft asphalt according to the ratio of 1:1.7, mix them evenly, put them into a settling tank for sedimentation, and finally separate the light phase and heavy phase; heat to 140°C when mixing, and then put it in a mixer and stir for 2 hours ;

[0037] S3. Heat the heavy phase obtained in S1 to 200°C, then pump it to the dehydration tower, separate the water in the dehydration tower, introduce it into the tube furnace, heat it to 310°C through the tube furnace, and introduce it into the distillation tower for distillation. The oil gas in the distillation becomes light oil after being cooled by the condensation tower, and the bitumen after distillation is discharged for standby;

[0038] S4. Heating the pitch prepared in S3 to 490° C. and then int...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle sizeaaaaaaaaaa
particle sizeaaaaaaaaaa
particle sizeaaaaaaaaaa
Login to View More

Abstract

The invention discloses a production method of needle coke, which comprises the following steps: S2, taking out the solvent and soft asphalt according to the ratio of 1:1.5-2, mixing them evenly, and separating the light phase and the heavy phase; S3, taking the S1 The heavy phase obtained in the process is heated to 150-200°C, separated from the water in the dehydration tower and then introduced into the tube furnace, heated to 300-360°C by the tube furnace, then introduced into the distillation tower for distillation, and the oil and gas in the distillation pass through the condensation tower After cooling, it becomes light oil, and the distilled asphalt is discharged for later use; S4, prepare coke; S5, take out the coke after cooling, and then crush it to particles with a particle size D50 not greater than 50mm, and mix coke, needle coke, and light oil according to the following weight The ratio of parts is taken out and mixed: 3‑4: 2‑3: 0.5‑1, heated to 150‑180°C during mixing, and stirred for 1‑2 hours; then filtered to retain the solid phase; S6, add Ni‑into the solid phase The Mo-based catalyst is then heated to 300-400° C. and maintained at an air pressure of 10-15Mpa, stirred for 1-2 hours, and taken out to obtain needle coke raw materials; S7, coke the needle coke raw materials.

Description

technical field [0001] The invention relates to needle coke preparation technology, in particular to a production method of needle coke. Background technique [0002] Needle coke is a high-quality variety that is vigorously developed among carbon materials. Its appearance is a silver-gray porous solid with metallic luster. The width ratio is like a fibrous or needle-like texture, and it feels smooth to the touch. It is a raw material for the production of high-end carbon products such as ultra-high-power electrodes, special carbon materials, carbon fibers and their composite materials. According to different production raw materials, needle coke can be divided into oil-based needle coke and coal-based needle coke. Needle coke produced with petroleum residue as raw material is oil-based needle coke; needle coke produced with coal tar pitch and its fractions as raw material is coal-based needle coke. [0003] At present, coal-based needle coke is mainly used in China, but th...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C10B55/00C10C3/00
CPCC10B55/00C10C3/00
Inventor 武建军
Owner 恒源碳材料股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products