A safe and reliable upper limb exercise device
An exercise device and a technology for upper limbs, applied in the field of physical exercise equipment, can solve problems such as poor safety performance, rotator cuff injury, affecting the quality of life of elderly users, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0060] The following is attached Figure 1-17 The present invention will be described in further detail.
[0061] A safe and reliable upper limb exercise device, such as Figure 1-17 As shown, a bottom plate 1 is included. Two sets of upper limb exercise units 2 are symmetrically provided on both sides of the upper part of the bottom plate 1, and the upper part of the bottom plate 1 is located between the two sets of upper limb exercise units 2 and a supporting unit 3 is provided;
[0062] The two sets of upper limb exercise units 2 each include a boss 6 fixedly mounted on the upper part of the bottom plate 1, and a sliding groove 7 is opened on the upper surface of the boss 6, and a sliding block is slidably installed inside the sliding groove 7 10. A vertical rod 11 is fixedly installed on the upper surface of the slider 10, a U-shaped bracket 12 is fixedly installed on the upper end of the vertical rod 11, and the upper part of the U-shaped bracket 12 is fixedly installed with a ...
Embodiment 2
[0074] The difference from Example 1 is that the handle 15 is also covered with a protective cover, and the protective cover is prepared by the following method:
[0075] Weigh the following raw materials in parts by weight: 30 parts of methyl vinyl phenyl silicone rubber, 15 parts of polyurethane, 10 parts of calcium carbonate powder, 15 parts of phenolic resin powder, 2 parts of p-phenylenediamine, 2 parts of triethanolamine Parts, 3 parts of paraffin oil, 3 parts of tricresyl phosphate;
[0076] S1. The weighed methyl vinyl phenyl silicone rubber and polyurethane are added to a pulverizer for pulverization. The rotation speed of the pulverizer is set to 600r / min to obtain a pulverized mixture, and the mixture is pulverized The diameter of the particles is 4mm;
[0077] S2. The pulverized mixture material prepared in step S1 is added to an internal mixer for banburying. The temperature of the internal mixer is set to 180°C, the rotation speed is set to 700r / min, and the banburying...
Embodiment 3
[0083] The difference from Example 2 is the preparation of the protective cover. The specific preparation method is as follows:
[0084] Weigh the following raw materials in parts by weight: 35 parts of methyl vinyl phenyl silicone rubber, 18 parts of polyurethane, 11 parts of calcium carbonate powder, 18 parts of phenolic resin powder, 3 parts of p-phenylenediamine, 3 parts of triethanolamine Parts, 4 parts of paraffin oil, 4 parts of tricresyl phosphate;
[0085] S1. The weighed methyl vinyl phenyl silicone rubber and polyurethane are added to a pulverizer for pulverization. The rotation speed of the pulverizer is set to 700 r / min to obtain a pulverized mixture, and the mixture is pulverized The diameter of the particles is 7mm;
[0086] S2. The pulverized mixture material obtained in step S1 is added to an internal mixer for banburying. The temperature of the internal mixer is set to 190°C, the rotation speed is set to 750r / min, and the banburying time is 30min. materials;
[008...