A technology of antifreeze and liquid level gauge, which is applied in the field of liquid level gauge, can solve the problems of poor heating efficiency of water jacket furnace, broken glass tube, heating and drying the pot, etc., and achieves the goal of avoiding freezing blockage and good heat preservation effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0053] Take 60 parts of polymethylene polyphenyl isocyanate, 30 parts of phenylenediamine polyether polyol, 36 parts of polyester ether polyol, 25 parts of catalyst, 20 parts of cyclopentane, 2.5 parts of active agent, 2 parts of deionized water 1 part, 4 parts of physical foaming agent were mixed uniformly in a stirring tank at 25°C with a stirring speed of 2800pm / min, and the resulting product was poured into a mold with a temperature of 45°C and left to stand for 3 to 4 minutes until the polymerization reaction was completed, that is Obtain the insulation material of the present invention.
[0054] The thermal insulation material of the present invention is prepared through polymerization reaction.
Embodiment 2
[0056] Take 60 parts of polymethylene polyphenyl isocyanate, 40 parts of phenylenediamine polyether polyol, 30 parts of polyester ether polyol, 15 parts of catalyst, 15 parts of cyclopentane, 2 parts of active agent, 1.5 parts of deionized water 1 part, 4 parts of physical foaming agent were mixed uniformly in a stirring tank at 25°C with a stirring speed of 2800pm / min, and the resulting product was poured into a mold with a temperature of 45°C and left to stand for 3 to 4 minutes until the polymerization reaction was completed, that is Obtain the insulation material of the present invention.
Embodiment 3
[0058] Take 60 parts of polymethylene polyphenyl isocyanate, 30 parts of phenylenediamine polyether polyol, 38 parts of polyester ether polyol, 25 parts of catalyst, 20 parts of cyclopentane, 2.5 parts of active agent, 2 parts of deionized water 1 part, 4 parts of physical foaming agent were mixed uniformly in a stirring tank at 25°C with a stirring speed of 2800pm / min, and the resulting product was poured into a mold with a temperature of 45°C and left to stand for 3 to 4 minutes until the polymerization reaction was completed, that is Obtain the insulation material of the present invention.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com