A technology for waste gas treatment and activated carbon powder, applied in separation methods, chemical instruments and methods, and other chemical processes, etc., can solve problems such as inability to fully satisfy, and achieve the effects of low cost, simple preparation method, and enhanced absorption rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The invention provides a high-activated carbon powder waste gas treatment material, which comprises the following materials in parts by weight: 51 parts of graphene, 30 parts of coconut shell activated carbon powder, 7 parts of nano silicon dioxide, 15 parts of polyvinylpyrrolidone, 5 parts of diatomaceous earth, poly 10 parts of vinyl alcohol, 20 parts of calcined kaolin, 4 parts of hydroxymethyl cellulose and 5 parts of cordierite;
[0026] Wherein, the preparation method / means of calcined kaolin comprises: calcining 100 mesh kaolin at a temperature of 600° C. for 3 hours to obtain calcined kaolin;
[0027] The preparation method of this exhaust gas treatment material comprises the following steps:
[0028] (1) Graphene, coconut shell activated carbon powder, nano silicon dioxide, polyvinylpyrrolidone, diatomaceous earth, calcined kaolin, hydroxymethylcellulose, cordierite are mixed and ground;
[0029] (2) Dissolve polyvinyl alcohol in 5 times of water, add the mixe...
Embodiment 2
[0032] The present invention provides a high-activated carbon powder waste gas treatment material, comprising the following materials in parts by weight: 53 parts of redox graphene, 31 parts of coconut shell activated carbon powder, 8.5 parts of nano silicon dioxide, 17.5 parts of polyvinylpyrrolidone, and 12.5 parts of diatomite , 11.5 parts of polyvinyl alcohol, 21 parts of calcined kaolin, 5.5 parts of hydroxymethyl cellulose and 7 parts of cordierite;
[0033] Wherein, calcining 150-mesh kaolin at a temperature of 700° C. for 3.5 hours to obtain calcined kaolin;
[0034] The preparation method of this exhaust gas treatment material comprises the following steps:
[0035] (1) redox graphene, coconut shell activated carbon powder, nano silicon dioxide, polyvinylpyrrolidone, diatomaceous earth, calcined kaolin, hydroxymethylcellulose, cordierite are mixed and ground;
[0036] (2) Dissolve polyvinyl alcohol in 5 times of water, add the mixed powder obtained in step (1), stir ...
Embodiment 3
[0039] The invention provides a high-activated carbon powder exhaust gas treatment material, which includes the following materials in parts by weight: 55 parts of graphene, 32 parts of coconut shell activated carbon powder, 10 parts of nano silicon dioxide, 20 parts of polyvinylpyrrolidone, 10 parts of diatomaceous earth, poly 13 parts of vinyl alcohol, 22 parts of calcined kaolin, 7 parts of hydroxymethyl cellulose and 9 parts of cordierite;
[0040] Wherein, the preparation method / means of calcined kaolin comprises: calcining 200 mesh kaolin at a temperature of 800° C. for 4 hours to obtain calcined kaolin;
[0041] The preparation method of this exhaust gas treatment material comprises the following steps:
[0042] (1) Graphene, coconut shell activated carbon powder, nano silicon dioxide, polyvinylpyrrolidone, diatomaceous earth, calcined kaolin, hydroxymethylcellulose, cordierite are mixed and ground;
[0043] (2) Dissolve polyvinyl alcohol in 6 times of water, add the m...
PUM
Property | Measurement | Unit |
---|---|---|
degree of polymerization | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com