Embodiment 1
[0032] A far-infrared plaster, which comprises the following raw materials in parts by weight: 90 parts of rubber paste, 0.03 part of far-infrared ceramic powder, 0.002 part of borneol, 0.002 part of ginger powder, and 0.002 part of moxa powder.
[0033] The preparation method specifically comprises the following steps:
[0034] Step 1: Weigh rubber paste, far-infrared ceramic powder, and borneol in proportion, add far-infrared ceramic powder and borneol after melting the rubber paste, and stir evenly to obtain a far-infrared material layer;
[0035] Step 2: Mix ginger powder and moxa powder evenly in proportion to obtain a mixture;
[0036] Step 3: coating the prepared far-infrared material layer on the base lining, and then spraying the mixture of ginger powder and mugwort powder evenly mixed on the far-infrared material layer, that is, a plaster is prepared on the base lining;
[0037] Step 4: Cover the plaster with a layer of release paper, divide it into strips, and slic...
Embodiment 2
[0039] A far-infrared plaster, which comprises the following raw materials in parts by weight: 100 parts of rubber paste, 0.06 part of far-infrared ceramic powder, 0.005 part of borneol, 0.005 part of ginger powder, and 0.005 part of moxa powder.
[0040] The preparation method specifically comprises the following steps:
[0041] Step 1: Weigh rubber paste, far-infrared ceramic powder, and borneol in proportion, add far-infrared ceramic powder and borneol after melting the rubber paste, and stir evenly to obtain a far-infrared material layer;
[0042] Step 2: Mix ginger powder and moxa powder evenly in proportion to obtain a mixture;
[0043] Step 3: coating the prepared far-infrared material layer on the base lining, and then spraying the mixture of ginger powder and mugwort powder evenly mixed on the far-infrared material layer, that is, a plaster is prepared on the base lining;
[0044]Step 4: Cover the plaster with a layer of release paper, divide it into strips, and slic...
Embodiment 3
[0046] A far-infrared plaster, said plaster comprising the following raw materials in parts by weight: 93 parts of rubber paste, 0.04 part of far-infrared ceramic powder, 0.003 part of borneol, 0.003 part of ginger powder, and 0.003 part of mugwort powder
[0047] The preparation method specifically comprises the following steps:
[0048] Step 1: Weigh rubber paste, far-infrared ceramic powder, and borneol in proportion, add far-infrared ceramic powder and borneol after melting the rubber paste, and stir evenly to obtain a far-infrared material layer;
[0049] Step 2: Mix ginger powder and moxa powder evenly in proportion to obtain a mixture;
[0050] Step 3: coating the prepared far-infrared material layer on the base lining, and then spraying the mixture of ginger powder and mugwort powder evenly mixed on the far-infrared material layer, that is, a plaster is prepared on the base lining;
[0051] Step 4: Cover the plaster with a layer of release paper, divide it into strips...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com