Method used for cleaning rock crystals and improving rock crystal surface machining precision
A surface processing and crystal technology, which is applied in the directions of cleaning methods, cleaning methods and utensils, chemical instruments and methods using liquids, etc., can solve the problems of increasing the production cost of enterprises, affecting the inspection of crystal chips, and poor crystal cleaning effect, etc. Accuracy, alleviating eye fatigue, good cleaning effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0041] Such as Figure 1-13 Shown, a kind of method that is used for crystal cleaning improves crystal surface processing precision, comprises the following steps:
[0042] a. Pre-cleaning: put the crystal wafer in pure water for ultrasonic or megasonic heating pre-cleaning;
[0043] b. Pickling: place the pre-cleaned crystal in hydrochloric acid solution for pickling;
[0044] c. Deacidification: put the pickled crystal in the crystal cleaning machine for cleaning to remove the acidic solution and dirt on the surface;
[0045] d. Drying: place the deacidified crystal wafers in a dryer for drying;
[0046] e. Inspection: Put the dried crystal chips into the crystal inspection device for inspection, and screen out the crystal chips with surface defects;
[0047] The temperature of the pure water used in step a is 60°C.
[0048] The concentration of hydrochloric acid used in step b is concentration 5%.
[0049] Crystal pickling time in step b is 20s.
[0050] In further de...
Embodiment 2
[0070] A method for improving crystal surface processing precision for crystal cleaning, comprising the following steps:
[0071] a. Pre-cleaning: put the crystal wafer in pure water for ultrasonic or megasonic heating pre-cleaning;
[0072] b. Pickling: place the pre-cleaned crystal in hydrochloric acid solution for pickling;
[0073] c. Deacidification: put the pickled crystal in the crystal cleaning machine for cleaning to remove the acidic solution and dirt on the surface;
[0074]d. Drying: place the deacidified crystal wafers in a dryer for drying;
[0075] e. Inspection: Put the dried crystal chips into the crystal inspection device for inspection, and screen out the crystal chips with surface defects;
[0076] The temperature of the pure water used in step a is 70°C.
[0077] The concentration of hydrochloric acid used in step b is concentration 20%.
[0078] Crystal pickling time in step b is 60s.