A high elastic thermal underwear chest ring
A high-elasticity, underwear technology, applied in bras, bras, clothing and other directions, can solve problems such as poor blood circulation and breathing effects, and achieve the effects of good resilience, increased support, and high memory effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] A high-elastic temperature-sensing underwear chest ring: including the following raw materials in parts by weight: 30 parts of quartz ore, 25 parts of nickel-titanium alloy, 12 parts of nano-titanium dioxide, and 12 parts of composite fiber; the composite fiber is composed of pineapple fiber, mushroom fiber, corn fiber Composition by mass ratio of 1:0.5:0.8;
Embodiment 2
[0020] A high-elastic temperature-sensing underwear chest ring: including the following raw materials in parts by weight: 50 parts of quartz ore, 34 parts of nickel-titanium alloy, 24 parts of nano-titanium dioxide, and 20 parts of composite fiber; the composite fiber is composed of pineapple fiber, mushroom fiber, corn fiber Composition by mass ratio of 3:1.6:2;
Embodiment 3
[0022] A high-elastic temperature-sensing underwear chest ring: including the following raw materials in parts by weight: 40 parts of quartz ore, 30 parts of nickel-titanium alloy, 18 parts of nano-titanium dioxide, and 16 parts of composite fiber; the composite fiber is composed of pineapple fiber, mushroom fiber, corn fiber Composed of 2:1:1.4 by mass ratio;
[0023] The above-mentioned embodiment 1-3 is a preparation method of a high-elastic temperature-sensitive underwear bra ring, comprising the following steps:
[0024] S1. Soak the composite fiber in propyl gallate solution for 5 hours according to the volume ratio of 1:3,
[0025] S2, grinding quartz ore and nano-titanium dioxide into powder, passing through a 160-mesh sieve;
[0026] S3. Heating the composite fiber to 60°C, pulverizing it, and passing it through a 400-mesh sieve;
[0027] S4. Mix the powders prepared by the above S1 and S2, and stir evenly to form a mixed powder. The stirring rate is 400r / min, and t...
PUM
Property | Measurement | Unit |
---|---|---|
yield strength | aaaaa | aaaaa |
elongation | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com