Supercharge Your Innovation With Domain-Expert AI Agents!

Composite sealing method for soft contact electromagnetic continuous casting mold slit

A continuous casting mold and composite sealing technology is applied in coating, fusion spraying, metal material coating technology and other directions to achieve the effects of good sealing, low cost and simple processing technology.

Active Publication Date: 2022-01-07
SHANGHAI UNIV
View PDF8 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

This sealing method effectively solves the problem of sealing the kerf of the full water-cooled soft-contact mold, avoids the safety hazard caused by the leakage of molten steel and the contact with cooling water, and at the same time meets the requirements of the high-frequency electromagnetic field on the insulation and magnetic conductivity of the copper tube of the mold. Requirements, with the advantages of high strength, high rigidity and good heat resistance, suitable for application in industrial production

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Composite sealing method for soft contact electromagnetic continuous casting mold slit
  • Composite sealing method for soft contact electromagnetic continuous casting mold slit
  • Composite sealing method for soft contact electromagnetic continuous casting mold slit

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] In this example, see Figure 1-3 , a soft-contact electromagnetic continuous casting mold slit compound sealing method, in which a hollow slit 3 is made on the mold wall 1, and then the slit 3 is cleaned and pretreated, and the hollowed slit 3 runs through the mold The inner and outer surfaces of the wall 1; filling material 14 is added in the middle of the slit 3, and the filling material 14 is a poor conductor of electricity, so that the filling material 14 fills the middle part of the slit 3, and the surface of the filling material 14 does not reach the slit 3 The surface of the crystallizer wall 1 in the direction of the opening forms a shallow groove; then continue to add sealing material 15 to the shallow groove until the shallow groove is filled, and the sealing material 15 adopts a material that can be firmly combined with the crystallizer matrix material; thereby making the surface of the sealing material 15 It is flush with the surface of the mold copper tube ...

Embodiment 2

[0030] The present embodiment is basically the same as the embodiment, and it is pointed out in particular that:

[0031] In the present embodiment, select the circular copper tube of pure copper crystallizer for use, and the diameter of the copper tube is 180mm, and the slit is started at 30mm below the top surface of the copper tube of the crystallizer; the slit 3 has a width of 1mm and a length of 150mm. There are 30 equidistant slits 3 in the circumferential direction, and the wall thickness of the copper pipe is 40mm. First, the slits 3 are cleaned and sandblasted, and thermal spraying is carried out by thermal spraying method, and then the middle part of the slit is sprayed and preheated to 1000°C ZrO 2 powder to make ZrO 2 The powder fills the middle part of the slit 3, the filling thickness d is 38mm, and the ZrO 2 The surface of the powder filling material does not reach the surface of the crystallizer wall in the direction of the opening of the slit, forming a shal...

Embodiment 3

[0034] This embodiment is basically the same as the previous embodiment, and it is particularly pointed out that:

[0035] In this example, see Figure 4 , a soft-contact electromagnetic continuous casting mold slit composite sealing method, making a non-hollow slit 3 on the mold wall 1, and the non-hollow slit 3 is a deep slit open toward the outer surface of the mold wall 1 Groove 16; then clean and pre-treat the slit 3, the hollow slit 3 runs through the inner and outer surfaces of the crystallizer wall 1; add a filling material 14 in the middle of the slit 3, and the filling material 14 is a poor conductor of electricity , make the filling material 14 fill up the middle part of the slit 3, and make the surface of the filling material 14 less than the surface of the crystallizer wall 1 in the opening direction of the slit 3, forming a shallow groove; then continue to add the sealing material 15 to the shallow groove until it is filled The shallow groove is full, and the se...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
widthaaaaaaaaaa
Login to View More

Abstract

The invention discloses a soft-contact electromagnetic continuous casting crystallizer slit compound sealing method, which adopts a cold spraying method, a thermal spraying method, or a welding method, and firstly adds a filling material in the middle of the slit, so that the filling material fills the slit Then add sealing materials from the inner cavity and outer wall of the copper tube of the crystallizer to the slit respectively. The added sealing materials are flush with the inner cavity wall and outer surface of the copper tube of the crystallizer respectively, so that the filling material, sealing material and crystallization The base body of the device is integrated into one body to realize the complete sealing of the split body and the incision. The invention has the advantages of simple implementation, good sealing performance, good magnetic permeability, easy processing and molding, low cost, and is suitable for industrial production and application.

Description

technical field [0001] The invention relates to a processing method of a soft-contact electromagnetic continuous casting crystallizer, in particular to a method for sealing a kerf of a soft-contact electromagnetic continuous casting mold, which is applied in the technical field of metallurgical equipment. Background technique [0002] Soft contact electromagnetic continuous casting technology is a new electromagnetic continuous casting technology. Its principle is to use the electromagnetic force generated by the high-frequency alternating magnetic field in the liquid metal to reduce the contact between the liquid metal and the mold wall, thereby effectively reducing or even eliminating crystallization. The purpose of the vibration mark defect on the surface of the slab caused by the vibration of the machine. [0003] The traditional continuous casting mold is usually composed of a whole copper conductor, but the copper material has a great shielding effect on the high-frequ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C23C24/04C23C4/11C23C4/08B22D11/049
CPCC23C24/04C23C4/11C23C4/08B22D11/049
Inventor 雷作胜卢海彪李彬孙晓辉李嘉勋
Owner SHANGHAI UNIV
Features
  • R&D
  • Intellectual Property
  • Life Sciences
  • Materials
  • Tech Scout
Why Patsnap Eureka
  • Unparalleled Data Quality
  • Higher Quality Content
  • 60% Fewer Hallucinations
Social media
Patsnap Eureka Blog
Learn More