Preparation method of antistatic composite fabric
A composite fabric and antistatic technology, applied in dyeing, fabric surface trimming, heating/cooling fabrics, etc., can solve the problems of wrapped conductive fibers that are not resistant to friction and repeated washing, poor fabric feel, and uncomfortable wearing, etc., to achieve Excellent antistatic performance, soft touch, and skin-friendly effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] The invention provides a technical solution: a method for preparing an antistatic composite fabric, comprising the following steps;
[0024] Step 1. Preparation of conductive fibers:
[0025] S1. Mix the antistatic modification liquid, hydrophilic softening agent and absolute ethanol according to a certain ratio to obtain solution A;
[0026] S2. Put the obtained solution A into an ultrasonic device and raise the temperature to 65° C., and process it for 35 minutes;
[0027] S3. Put the fiber into the ultrasonic equipment and mix it with solution A, start the ultrasonic equipment, and then raise the temperature by 5°C every 2 minutes until 55°C for 25 minutes to obtain antistatic fibers;
[0028] The fiber is a blend of acrylic fiber and bamboo fiber;
[0029] The ratio of antistatic modifying solution, hydrophilic softening agent and absolute ethanol is 3:1:5, stir by magnetic force for 2 hours, filter the obtained solution, and take the filtrate;
[0030] Step 2. W...
Embodiment 2
[0037] The invention provides a technical solution: a method for preparing an antistatic composite fabric, comprising the following steps;
[0038] Step 1. Preparation of conductive fibers:
[0039] S1. Mix the antistatic modification liquid, hydrophilic softening agent and absolute ethanol according to a certain ratio to obtain solution A;
[0040] S2. Put the obtained solution A into the ultrasonic equipment and raise the temperature to 70° C., and process it for 32 minutes;
[0041] S3. Put the fibers into the ultrasonic equipment and mix them with solution A, start the ultrasonic equipment, then raise the temperature by 5°C every 2-3min until 50-60°C, and last for 15-30min to obtain antistatic fibers;
[0042] The fiber is PAN fiber;
[0043] The ratio of antistatic modifying solution, hydrophilic softening agent and absolute ethanol is 3:1:5, stir by magnetic force for 2 hours, filter the obtained solution, and take the filtrate;
[0044] Step 2. Wash the obtained anti...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com