Fever cooling patch gel and preparation method thereof
A cooling patch and gel technology, which is applied in the field of gel for cooling patch and its preparation, can solve the problems of troublesome mass production, inconsistent urea content, high solubility of urea, etc., and achieve the effect of good heat absorption and cooling, and good quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A gel for antipyretic plasters, which contains a polymer, a liquid dispersion medium, and urea, and the urea content is its solubility at 40°C; the solubility of urea at 40°C is 129g of urea dissolved in 100g of water.
[0028] The pH of the gel was 8.2.
[0029] The liquid dispersion medium is a buffer solution, and the buffer solution is a barbital sodium-hydrochloric acid buffer solution with a pH of 8.2.
[0030] The polymer is carbomer.
[0031] The gel is carried out according to the following steps: the buffer solution is heated to 40° C. and maintained;
[0032] Add urea to dissolve urea;
[0033] Add carbomer, the amount of carbomer added is 1 / 20 of water, keep the temperature constant, add 10% sodium hydroxide solution, until the pH value is 8.2, stir, and gel.
Embodiment 2
[0035] A gel for antipyretic plasters, which contains a polymer, a liquid dispersion medium, and urea, and the urea content is its solubility at 40°C; the solubility of urea at 40°C is 129g of urea dissolved in 100g of water.
[0036] The pH of the gel was 8.2.
[0037] The liquid dispersion medium is water.
[0038] The polymer is carbomer.
[0039] The gel is carried out according to the following steps: heat the water to 40°C and keep it;
[0040] Add urea to dissolve urea;
[0041] Add carbomer, the amount of carbomer added is 1 / 20 of water, keep the temperature constant, add 10% sodium hydroxide solution, until the pH is 8.2, stir, gel.
Embodiment 3
[0043] A gel for antipyretic plasters, which contains a polymer, a liquid dispersion medium, and urea, and the urea content is its solubility at 40°C; the solubility of urea at 40°C is 129g of urea dissolved in 100g of water.
[0044] The liquid dispersion medium is water; the polymer is gelatin.
[0045] The gel is carried out according to the following steps: heat the water to 40°C and keep it;
[0046] Add urea to dissolve urea;
[0047] Add gelatin, the amount of gelatin added is 2 / 1000 of water, stir to obtain a mixture;
[0048] Let cool and the mixture gels within a minute.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More