Celadon justice cup and firing method thereof
A fair cup and celadon technology, applied in the field of celadon fair cup and its firing, can solve problems such as damage of fair cup and loss of use value, and achieve the effects of improving aesthetics, improving interest and good effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0042] Such as Figure 1~3 A celadon justice cup is shown, which includes a cup body 1 and a cup holder 2 arranged below the cup body 1. The inside of the side wall of the cup body 1 is provided with at least one inverted U-shaped through groove 3. One end of the inverted U-shaped channel 3 communicates with the bottom end of the side wall of the cup body 1 to form a water inlet 4, and the other end of the inverted U-shaped channel 3 passes downward through the side wall of the cup body 1 to form a water outlet 5. The water outlet 5 is arranged inside the cup holder 2 .
Embodiment 2
[0044] Such as Figure 1~4As shown, a celadon justice cup includes a cup body 1 and a cup holder 2 arranged under the cup body 1. The inside of the side wall of the cup body 1 is provided with at least one inverted U-shaped through groove 3, so One end of the inverted U-shaped through groove 3 communicates with the bottom end of the side wall of the cup body 1 to form a water inlet 4, and the front end of the water inlet 4 is provided with a piece of filter ceramic block 6, and the surface is uniformly distributed with diameters of 0.1~1mm. A small through hole 7 , the other end of the inverted U-shaped through groove 3 passes downwards through the side wall of the cup body 1 to form a water outlet 5 , and the water outlet 5 is arranged inside the cup holder 2 .
Embodiment 3
[0046] A firing method of a celadon justice cup, the firing method comprising the following steps:
[0047] (S.1) Slurry preparation: Grind and sieve kaolin and mix it with water at a weight ratio of 100:30, then add 0.1% organosilicon powder, 0.1% sodium borosilicate, diatomaceous earth in kaolin mass percentage 1% and polyethylene glycol 4000 0.5%, after being stirred evenly, china clay slurry is obtained;
[0048] (S.2) Shaping: shaping the obtained slurry to obtain a cup embryo;
[0049] (S.3) Buried pipe: bury 1 inverted U-shaped soft plastic pipe made of polyethylene on the inner wall of the obtained cup embryo, so that one end of the plastic pipe penetrates the inner wall of the cup embryo to form a water inlet, and the other end is downward Pass through the cup body and set an outlet pipe made of slurry on the outside, and connect it with the cup body to form a water outlet, and obtain a fair cup embryo body after drying;
[0050] (S.4) Biscuit firing: Bisque firing ...
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com