Pressure vessel head with buffering function and buffering method thereof
A technology of pressure vessel and buffer method, applied in pressure vessels, fixed-capacity gas storage tanks, material gluing, etc., can solve problems such as damage to the surface quality of the head, shorten the service life of the head, and have no buffer performance, and achieve the protection of quality , Improve the economic benefits of production and processing, the effect is remarkable
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A pressure vessel head with a buffer function and a buffer method thereof, comprising the following steps:
[0028] S1. Sandblasting: Use a sandblasting machine to perform sandblasting on the surface of the pressure vessel head, and then let it stand for 30 minutes;
[0029] S2. Cleaning and dust removal: put the pressure vessel head in step S1 into No. 100 gasoline, stir and clean for 60 minutes;
[0030] S3, drying: put the pressure vessel head in step S2 into an oven, set the temperature to 120°C, and heat for 45 minutes;
[0031] S4. Applying: apply a layer of adhesive on the surface of the pressure vessel head in step S3;
[0032] S5. Vulcanization: The styrene-butadiene rubber is vulcanized. The vulcanization steps mainly include induction-pre-vulcanization-normal vulcanization-overvulcanization, and the vulcanization temperature is 100°C.
[0033] S6. Adhesive finished product: Cover the vulcanized rubber in step S5 on the head of the pressure vessel in step S3...
Embodiment 2
[0038] A pressure vessel head with a buffer function and a buffer method thereof, comprising the following steps:
[0039] S1. Sandblasting: Use a sandblasting machine to perform sandblasting on the surface of the pressure vessel head, and then let it stand for 30 minutes;
[0040] S2. Cleaning and dust removal: put the pressure vessel head in step S1 into No. 100 gasoline, stir and clean for 60 minutes;
[0041] S3, drying: put the pressure vessel head in step S2 into an oven, set the temperature to 120°C, and heat for 45 minutes;
[0042] S4. Applying: apply a layer of adhesive on the surface of the pressure vessel head in step S3;
[0043] S5. Vulcanization: The styrene-butadiene rubber is vulcanized. The vulcanization steps mainly include induction-pre-vulcanization-normal vulcanization-overvulcanization, and the vulcanization temperature is 160°C.
[0044] S6. Adhesive finished product: cover the vulcanized rubber in step S5 on the head of the pressure vessel in step S3...
Embodiment 3
[0049] A pressure vessel head with a buffer function and a buffer method thereof, comprising the following steps:
[0050] S1. Sandblasting: Use a sandblasting machine to perform sandblasting on the surface of the pressure vessel head, and then let it stand for 30 minutes;
[0051] S2. Cleaning and dust removal: put the pressure vessel head in step S1 into No. 100 gasoline, stir and clean for 60 minutes;
[0052] S3, drying: put the pressure vessel head in step S2 into an oven, set the temperature to 120°C, and heat for 45 minutes;
[0053] S4. Applying: apply a layer of adhesive on the surface of the pressure vessel head in step S3;
[0054] S5. Vulcanization: The styrene-butadiene rubber is vulcanized. The vulcanization steps mainly include induction-pre-vulcanization-normal vulcanization-overvulcanization, and the vulcanization temperature is 120°C.
[0055] S6. Adhesive finished product: cover the vulcanized rubber in step S5 on the head of the pressure vessel in step S3...
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |