Preparation method of mirror release paper for leather
A technology for release paper and leather, which is applied in the field of preparation of mirror release paper for leather, and achieves the effects of quality stability assurance, rapid cooling and solidification, and whitening avoidance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0025] The present invention provides a kind of preparation method of mirror release paper for leather, comprising the following steps:
[0026] S1: Provide the base paper 10, the coating material and the coating machine, the coating machine includes a mirror roll 20 with a smooth surface, an auxiliary roll 40 in contact with the surface of the mirror roll 20, and an auxiliary roll 40 located at the upper end of the mirror roll 20 Laminating head 30, such as figure 1 As shown; the coating material includes the following components by weight: 58 parts-62 parts of polypropylene, 38 parts-42 parts of polyethylene;
[0027] S2: Place the base paper 10 between the mirror roller 20 and the auxiliary roller 40, pour the coating material between the mirror roller 20 and the base paper 10 through the coating head 30, and pass the mirror roller 20 to the base paper 10 coated with the coating material Apply pressure to form a coating material layer with a smooth surface on the surface o...
Embodiment 1
[0042] A preparation method for mirror surface release paper for leather, comprising the steps of:
[0043] S1: Provide the base paper 10, the coating material and the coating machine, the coating machine includes a mirror roll 20 with a smooth surface, an auxiliary roll 40 in contact with the surface of the mirror roll 20, and an auxiliary roll 40 located at the upper end of the mirror roll 20 Laminating head 30; the laminating material includes the following components by weight: 60 parts of polypropylene and 40 parts of polyethylene; the quality index requirements of the mirror roller 20 are: surface hardness is HRc60-HRc70, and balance is G40 Grade, smoothness is Ra0.02-Ra0.006, roughness is Ra0.8-Ra1.0;
[0044]S2: Place the base paper 10 between the mirror roller 20 and the auxiliary roller 40, pour the coating material between the mirror roller 20 and the base paper 10 through the coating head 30, and pass the mirror roller 20 to the base paper 10 coated with the coatin...
Embodiment 2
[0046] A preparation method for mirror surface release paper for leather, comprising the steps of:
[0047] S1: Provide the base paper 10, the coating material and the coating machine, the coating machine includes a mirror roll 20 with a smooth surface, an auxiliary roll 40 in contact with the surface of the mirror roll 20, and an auxiliary roll 40 located at the upper end of the mirror roll 20 Laminating head 30; The coating material package Comprising the following components by weight: 58 parts of polypropylene, 38 parts of polyethylene; The quality index requirements of the mirror roller 20 are: the surface hardness is HRc60-HRc70, the balance is G40, the smoothness is Ra0.02-Ra0.006, and the roughness is Ra0.8-Ra1.0;
[0048] S2: Place the base paper 10 between the mirror roller 20 and the auxiliary roller 40, pour the coating material between the mirror roller 20 and the base paper 10 through the coating head 30, and pass the mirror roller 20 to the base paper 10 coat...