A soil pollution and mine technology, applied in the field of soil pollution remediation of rare earth mines, can solve the problems of large influence and limitation on the living and growing environment of microorganisms, and achieve the effects of reducing costs, realizing recycling and improving soil physical and chemical properties.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0015] Add 40 parts of calcium phosphate, 40 parts of potassium nitrate, 40 parts of calcium nitrate, 30 parts of limestone, 30 parts of coal powder ash, and 2 parts of borax into water, mix well, and form a solution to obtain a mixed solution. 40 parts of rice straw, 35 parts of peach leaves, 25 parts of dried edamame sprouts, 16 parts of cow dung, 14 parts of plant ash, and 10 parts of chitosan are placed in a mixing mixer and mixed to obtain a mixture, and then added to obtain mixed solution, mixed evenly, left standstill, and dried to obtain a semi-finished product, 120 parts of humus and semi-finished product were mixed evenly to obtain a composition, and the composition was evenly sprinkled on the surface of the mine soil to make the composition and the surface of the mine The soil is mixed evenly, and the lentil magnei is put in the soil, and then the horseshoe is planted, and the water is sprayed on the surface of the soil, and the moisture content of the soil is 20-40%...
Embodiment 2
[0017] Add 40 parts of calcium phosphate, 40 parts of potassium nitrate, 40 parts of calcium nitrate, 30 parts of limestone, 30 parts of coal powder ash, and 2 parts of borax into water, mix well, and form a solution to obtain a mixed solution. 40 parts of rice straw, 35 parts of peach leaves, 25 parts of dried edamame sprouts, 16 parts of cow dung, 14 parts of plant ash, and 10 parts of chitosan are placed in a mixing mixer and mixed to obtain a mixture, and then added to obtain mixed solution, mixed evenly, left standstill, and dried to obtain a semi-finished product, 120 parts of humus and semi-finished product were mixed evenly to obtain a composition, and the composition was evenly sprinkled on the surface of the mine soil to make the composition and the surface of the mine Mix the soil evenly, spray water on the surface of the soil, and make the moisture content of the soil 20-40%.
Embodiment 3
[0019] Put 40 parts of rice straw, 35 parts of peach leaves, 25 parts of dried edamame sprouts, 16 parts of cow dung, 14 parts of plant ash, and 10 parts of chitosan in a mixing mixer to obtain a mixture, and then add The mixed solution obtained is mixed uniformly, left standing, and dried to obtain a semi-finished product, and 120 parts of humus and semi-finished product are mixed uniformly to obtain a composition, and the composition is evenly sprinkled on the surface of the mine soil to make the composition and the mine The surface soil is mixed evenly, and the lentil bean worm is put into the soil, and then the horseshoe is planted, and water is sprayed on the surface of the soil, and the moisture content of the soil is 20-40%.
PUM