Preparation method of composite organic high-water-holding-capacity culture medium material
A matrix material and composite technology, applied in planting substrates, botanical equipment and methods, cultivation and other directions, can solve the problems of difficult large-scale production, complex formula, difficult processing, etc. The effect of promoting flowering and fruiting
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] Step 1: The selected polyvinyl alcohol model is PVA-1799, the degree of polymerization is 1700, and the degree of alcoholysis is 99%;
[0026] Wood flour is composted from miscellaneous wood or landscaping waste, crushed and passed through a 200-mesh sieve;
[0027] Foaming agent is sodium lauryl sulfate;
[0028] The cross-linking agent is borax, and the main component is sodium tetraborate.
[0029] Get wood powder 12g, water 55ml, make wood powder aqueous solution;
[0030] Get whipping agent 0.08g, water 5ml, make foaming agent aqueous solution;
[0031] Take 0.67 g of the crosslinking agent and 5 ml of water to prepare an aqueous solution of the crosslinking agent.
[0032] Step 2: Take 4g of polyvinyl alcohol and 23ml of water to mix polyvinyl alcohol and water. Heating in a water bath at 90-100°C and stirring at a speed of 100r / min for 0.5h to obtain an aqueous solution of polyvinyl alcohol;
[0033] Step 3: Lower the polyvinyl alcohol aqueous solution to a ...
Embodiment 2
[0036] Step 1: Select the required polyvinyl alcohol, wood flour, foaming agent, crosslinking agent, and water.
[0037] Get wood powder 8g, water 35ml, make wood powder aqueous solution;
[0038] Get whipping agent 0.08g, water 5ml, make foaming agent aqueous solution;
[0039] Take 0.67 g of the crosslinking agent and 5 ml of water to prepare an aqueous solution of the crosslinking agent.
[0040] Step 2: Take 8g of polyvinyl alcohol and 45ml of water to mix polyvinyl alcohol and water. Heating in a water bath at 90-100°C and stirring at a speed of 100r / min for 0.5h to obtain an aqueous solution of polyvinyl alcohol.
[0041] Step 3: Lower the polyvinyl alcohol aqueous solution to a temperature of 60° C., add wood flour aqueous solution and foaming agent aqueous solution, and stir evenly.
[0042] Step 4: Add the cross-linking agent aqueous solution dropwise to the above mixed solution, stir at 1700-1800r / min for 3 minutes, the solution foams to 2.5 times the original vol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com