Grind grading technique for aluminum oxide raw material - monohydrallite
A process technology, bauxite technology, which is applied in the field of refining process of alumina raw material bauxite, can solve the problems of difficult management and operation, many equipments, complicated process flow, etc., and achieve simplified grinding process, Effect of reducing power consumption and improving equipment operation rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Embodiment 1: Add bauxite and lime in proportion to the double-chamber overflow type ball mill through the grinding head bin and feeder, and add a small amount of circulating mother liquor in the mill. According to the different characteristics of bauxite, The dosage of lime is usually between 5% and 23% of the weight of bauxite, and the dosage of circulating mother liquor is in the range of 0.8 to 1.1 based on the grinding liquid-solid ratio L / S. After the bauxite is coarsely ground in the first warehouse, it enters the second warehouse for fine grinding. The finely ground slurry enters the hydrocyclone for classification, and the bottom flow of the classification is coarse sand and returns to the mill. The pulp is pumped into the raw pulp tank. The main technical parameters in the process are as follows:
[0018] — Grinding liquid-solid ratio: L / S 0.8~1.1;
[0019] — Grinding temperature: 70-90°C;
[0020] —The amount of sand returned by the mill: 150% to 250%;
...
Embodiment 2
[0027] Embodiment 2: A grinding device for producing alumina by using bauxite. According to the characteristics of the ore, no lime is added in the grinding process, or only 1% to 4% of the weight of the bauxite is added. The technical indicators are as follows :
[0028] — Grinding liquid-solid ratio: L / S 0.8~1.1;
[0029] — Grinding temperature: 70-90°C;
[0030] —The amount of sand returned by the mill: 200% to 250%;
[0031] - Bauxite feed grain size: 12 ~ 40mm;
[0032] - Raw pulp product fineness: 100%<48 mesh, 95%<65 mesh, 42%~50%<325 mesh;
[0033] —Classification pressure of hydrocyclone: 0.08~0.15MPa;
[0034] - Solid content of hydrocyclone feed: 300-450g / L;
[0035] —Solid content of hydrocyclone overflow: 280~380g / L;
[0036] —Solid content in the bottom fluid of hydrocyclone: 900~1200g / L.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com