Composition of 5RP 8.5/4 pigment and practicality color block prepared by the same
A composition and pigment technology, applied in the direction of pigment-containing coatings, coatings, etc., can solve problems such as inaccurate control, and achieve strong practical value, high accuracy, and good ratio reproducibility
- Summary
 - Abstract
 - Description
 - Claims
 - Application Information
 
 AI Technical Summary 
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] Weigh 5.15 grams of PV19, 0.34 grams of PR101, and 1000 grams of CSC-A base material. Mix the above raw materials, and then apply the mixed composition evenly and evenly on the coated paper under the environmental conditions of relative humidity of 50%±5% and room temperature of 23±2°C. The wet film thickness of the coating is 250 μm, and then placed in a precision oven at 50±2°C for 3 to 4 hours to constant weight, taken out, cooled to room temperature, and obtained a physical color block.
Embodiment 2
[0023] Embodiment 2: Weigh 5.11 grams of PV19, 0.33 grams of PR101, and 1000 grams of CSC-A base material. Manufacturing process is with embodiment 1.
Embodiment 3
[0024] Embodiment 3: Weigh 5.19 grams of PV19, 0.34 grams of PR101, and 1005 grams of CSC-A base material by weight. Manufacturing process is with embodiment 1.
PUM
| Property | Measurement | Unit | 
|---|---|---|
| particle size | aaaaa | aaaaa | 
| minimum film forming temperature | aaaaa | aaaaa | 
| glass transition temperature | aaaaa | aaaaa | 
Abstract
Description
Claims
Application Information
 Login to View More - R&D
 - Intellectual Property
 - Life Sciences
 - Materials
 - Tech Scout
 
- Unparalleled Data Quality
 - Higher Quality Content
 - 60% Fewer Hallucinations
 
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com