Solid phase catalytic auxiliary and its preparation method and use
A technology of additives and catalysts, applied in chemical instruments and methods, physical/chemical process catalysts, organic compounds/hydrides/coordination complex catalysts, etc., to improve Fenton reaction efficiency, increase rate, and reduce operating costs Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0053] Take 10 g of strongly basic anion exchange resin (Amberlite IRA 900 type, Aldrich Reagent Company, USA) with styrene / divinylbenzene with a selected particle size of 1.0-1.5 mm as a copolymer, and pickle with hydrochloric acid. After alkali washing with sodium hydroxide, add it to the reaction vessel, stir, slowly add Alizarin Violet 3B aqueous solution (500mL, 76mmol) for loading, continue stirring for 20 hours after the addition is complete, and stop stirring. Rinse with water until there is no purple color in the solution, filter, and dry at 20°C for 40 hours to obtain the catalytic assistant.
Embodiment 2
[0055] Take 10g of strong basic anion exchange resin (Amberlite IRA 900 type of Aldrich Reagent Company, USA) with styrene / divinylbenzene having a selected particle size of 1.0-1.5mm as a copolymer, after acid washing and After alkali washing treatment, it was added to the reaction vessel, and under stirring, an aqueous solution of alizarin red (500 mL, 76 mmol) was slowly added for loading, and stirring was continued for 25 hours. Rinse with water until there is no red color in the solution, filter, and dry at 40°C for 45 hours at a low temperature to obtain a catalytic assistant.
Embodiment 3
[0057] Take 10 g of styrene / divinylbenzene with a selected particle size of 1.0-1.5 mm as a copolymer of strong basic anion exchange resin with quaternary ammonium groups (Amberlite IRA 900 type, Aldrich Reagent Company, USA) and wash with acid and alkali After the treatment, it was added to the reaction vessel, stirred, and the No. 2 orange solution was slowly added for loading (500 mL, 76 mmol), and stirred for 28 hours. Rinse with water until there is no color in the solution, filter, and dry at 60°C for 45 hours to obtain a catalyst promoter.
PUM
| Property | Measurement | Unit |
|---|---|---|
| wavelength | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |
| particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 