Embodiment 1
[0013] Add 0.1 part of polyacrylamide, 0.2 part of ethylene oxide, 0.5 part of diesel oil demulsifier by weight components, and the rest is sodium sulfate. Add 1 mol / l sulfuric acid to control the pH value at 3. Stir and mix evenly to obtain a composite demulsifier. The method of use is as follows: add 3% demulsifier to the diesel alkali slag by weight percentage, fully mix at 60°C, and after standing for 2 hours, the oil-water layer becomes clear.
Embodiment 2
[0015] Add 0.2 parts of polyacrylamide, 0.4 parts of ethylene oxide, 1 part of diesel oil demulsifier by weight components, and the rest is sodium sulfate. Add 1 mol / l sulfuric acid to control the pH value at 3.5. Stir and mix evenly to obtain a composite demulsifier. The method of use is as follows: add 8% demulsifier to the diesel alkali slag by weight percentage, fully mix at 70°C, and after standing for 5 hours, the oil-water layer becomes clear.
Embodiment 3
[0017] Add 0.3 parts of polyacrylamide, 0.6 parts of ethylene oxide, 2 parts of diesel oil demulsifier by weight components, and the rest is sodium sulfate. Add 1 mol / l sulfuric acid dropwise to control the pH value at 4. Stir and mix evenly to obtain a composite demulsifier. The method of use is as follows: add 4% demulsifier to the diesel alkali slag by weight percentage, fully mix at 50 DEG C, and after standing for 4 hours, the oil-water layer becomes clear.