A production method and a coat rack technology, which are applied in the field of automobile interior parts, can solve the problems of inability to meet the shape requirements of the coat rack, large shrinkage deformation, thin thickness, etc., and achieve the effects of not easily deformed, reducing weight, and high rigidity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] Embodiment one: the production method of a kind of automobile coat rack (rear shelf) of the present invention adopts following processing steps:
[0017] Parts specifications: L1200×W580×H5mm; use natural hemp fiberboard as the base of the coat rack.
[0018] 1. Board body drying temperature softening treatment: Put the hemp fiber board into a double-oven suspended oven for softening treatment (the rated temperature of the oven is 400°C), the temperature of the upper and lower heating zones is 230°C, and after the softening treatment is pre-heated for 60-80s, Continue the main heating for 90-110 seconds.
[0019] 2. Compression forming: Press and form the above-mentioned softened hemp fiber board, forming time: 50s, forming pressure: 100kgf / cm 2 .
[0020] 3. Cooling and shaping: The semi-finished product after pressing is cooled and shaped at room temperature, and the cooling time is 75s.
[0021] 4. Fabric lamination: Put the formed semi-finished product and needle...
Embodiment 2
[0024] Embodiment two: the production method of a kind of automobile coat rack (rear shelf) of the present invention adopts the following process steps: part specification: L1200 * W580 * H5mm, selects natural hemp fiber board for use as the substrate of coat rack.
[0025] 1. Board body drying temperature softening treatment: Put the hemp fiber board into the double oven suspended oven for softening treatment (the rated temperature of the oven is 400°C), the temperature of the upper and lower heating zones is 250°C, and the preheating time for drying temperature: 70s, the main Heating time: 100s.
[0026] 2. Press forming: Press and form the above softened hemp fiber board, press forming time: 60s, forming pressure: 100kgf / cm 2 .
[0027] 3. Cooling and shaping: Cool and shape the pressed semi-finished product at room temperature, cooling time: 80s.
[0028] 4. Fabric lamination: Laminate the above-mentioned semi-finished products with needle-punched non-woven fabrics. The ...
Embodiment 3
[0031] Embodiment three: the production method of a kind of automobile coat rack (rear shelf) of the present invention adopts the following process steps: part specification: L1200 * W580 * H5mm, selects natural hemp fiber board for use as the substrate of coat rack.
[0032] 1. Board body drying temperature softening treatment: put the hemp fiber board into the double-oven suspended oven for softening treatment (the rated temperature of the oven is 400 ° C), the temperature of the upper and lower heating zones is 270 ° C, the drying time is , and the pre-heating time is: 80s, main heating time: 110s.
[0033] 2. Compression forming: Press and form the above-mentioned softened hemp fiberboard, forming time: 70s, forming pressure: 100kgf / cm 2 .
[0034] 3. Cooling and shaping: The semi-finished product after pressing is cooled and shaped at room temperature, and the cooling time is 95s.
[0035] 4. Fabric lamination: Laminate the above-mentioned semi-finished products with ne...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com