Method for manufacturing fluorescent metal ceiling
A production method and ceiling technology, applied in the direction of luminescent paint, a device for coating liquid on the surface, and a process for producing decorative surface effects, etc., can solve the problem that the decorative board cannot emit light, etc., and achieve low manufacturing cost and simple production method , the effect of adding interest to life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] Fluorescent metal ceilings can use various types of ceiling materials as substrates, such as surface-treated (painted or oxidized) metal ceiling materials, traditional spray-coated or roll-coated metal ceiling materials, and film-coated ceiling materials. According to the substrate and pattern requirements, select the appropriate pattern layer ink or paint, and use the screen to coat the pattern layer. Then prepare the luminous solvent, choose alkyd ink 12-70B synthetic fatty acid alkyd resin as the film-forming material, C type 20-40 light green luminous powder pigment, the amount of luminous powder is 20% of the total weight of the luminous solvent, or 20% of the total weight of the luminous solvent 10% of solvent volume. Add the luminous powder and ink in proportion to PE and other plastic containers for high-speed dispersion and stirring, and the viscosity is controlled at 3000 poise. Viscosity was controlled using xylene dilution.
[0015] Then, the luminous laye...
Embodiment 2
[0017] Fluorescent metal ceilings can use various types of ceiling materials as substrates, such as surface-treated (painted or oxidized) metal ceiling materials, traditional spray-coated or roll-coated metal ceiling materials, and film-coated ceiling materials. To prepare the luminous solvent, select propionic acid paint butyl acrylate as the film-forming substance, D-type 10-15 yellow-green luminous powder pigment, and the amount of luminous powder is 40% of the total weight of the luminous solvent, or 20% of the volume of the luminous solvent. Add the luminous powder and paint in proportion to the container with glass and enamel lining for high-speed dispersion and stirring, and the viscosity is controlled at 4000 poise. Viscosity was controlled using methanol dilution.
[0018] Then, the luminous layer is coated with a screen of less than 200 meshes, and the thickness of the luminous layer is 125um. Then apply an abrasion-resistant protective layer and finish with a water...
Embodiment 3
[0020] Fluorescent metal ceilings can use various types of ceiling materials as substrates, such as surface-treated (painted or oxidized) metal ceiling materials, traditional spray-coated or roll-coated metal ceiling materials, and film-coated ceiling materials. According to the substrate and pattern requirements, select the appropriate pattern layer ink or paint, and coat the pattern layer with a screen of 200 mesh or less. Then prepare the luminous solvent, select WSR-120 acrylic modified epoxy resin as the film-forming material, E-type 5-10 yellow luminous powder pigment, the amount of luminous powder is 60% of the total weight of the luminous solvent, or 35% of the volume of the luminous solvent %. Add the luminous powder and paint in proportion to the container with glass and enamel lining for high-speed dispersion and stirring, and the viscosity is controlled at 5000 poise. In order to fully mix the luminous powder and the master agent evenly, an appropriate amount of S...