A kind of antirust liquid for inner cavity of parts
A technology of anti-rust liquid and inner cavity, applied in the direction of metal material coating process, etc., can solve the problems of slow rust removal, cannot be applied to large-scale production of automobiles, and cannot meet the needs of large-scale production of automobiles, and achieves the effect of saving costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] 1.5 parts has the molecular formula C 6 h 18 o 24 P 6 An organic acid, 8 parts of triethanolamine, 5 parts of refined petroleum sodium sulfonate, 40 parts of tap water, heated and stirred at 50°C for 10 minutes to form a relatively viscous liquid, and gradually added 3 parts of fatty alcohol polyoxyethylene Ether AEO3 causes a transparent viscous liquid, continue heating and stirring, add 0.1 part of polyethylene glycol 6000 distearate, 0.5 part of citric acid, 5 parts of triethanolamine, 0.5 part of industrial alcohol, 500ppm industrial Cathone Bactericide, add the remaining 36.9 parts of tap water, and finally add 1 part of sodium molybdate, and use 0.1 part of sodium hydroxide to adjust the pH value of the antirust solution to 9.0 transparent liquid.
Embodiment 2
[0023] 4.5 parts have the molecular formula C 6 h 18 o 24 P 6 An organic acid, 10 parts of triethanolamine, 12 parts of refined petroleum sodium sulfonate, 40 parts of tap water, heated and stirred at 55°C for 10 minutes to form a relatively viscous liquid, and gradually added 4 parts of fatty alcohol polyoxyethylene Ether AEO3 causes a transparent viscous liquid, continue heating and stirring, add 0.5 parts of polyethylene glycol 6000 distearate, 3.5 parts of citric acid, 8 parts of triethanolamine, 1 part of industrial alcohol, 500ppm industrial Cathone Bactericide, add the remaining 20 parts of tap water, and finally add 0.5 parts of sodium molybdate, and use 0.5 parts of sodium hydroxide to adjust the pH value of the antirust solution to 9.0 transparent liquid.
Embodiment 3
[0025] 2.5 parts has the molecular formula C 6 h 18 o 24 P 6 An organic acid, 10 parts of triethanolamine, 10 parts of refined petroleum sodium sulfonate, 40 parts of tap water, heated and stirred at 60°C for 10 minutes to form a relatively viscous liquid, and gradually added 3 parts of fatty alcohol polyoxyethylene Ether AEO3 causes a transparent viscous liquid. Continue heating and stirring to add 0.3 parts of macrogol 6000 distearate, 1 part of citric acid, 6 parts of triethanolamine, 0.8 parts of industrial alcohol, and 300 ppm of industrial Cathone Bactericide, add the remaining 24.5 parts of tap water, and finally add 1.5 parts of sodium molybdate, and adjust the pH value of the antirust solution to 9.0 transparent liquid with 0.4 parts of sodium hydroxide.