Embodiment 1
[0007] A preparation method of lampshade glass coating, the steps of the method are as follows: 1) Weigh the following materials in parts by weight: 20 parts of octamethylcyclotetrasiloxane, 20 parts of acrylic acid, 13 parts of ethanol, 20 parts of polyethylene oxide Ethylene, 2 parts of xylene and 15 parts of dimethyl phthalate; 2) Mix the above materials and stir at a constant temperature of 45°C for 5 hours to obtain a glass coating.
Embodiment 2
[0009] A method for preparing a lampshade glass coating. The steps of the method are as follows: 1) Weigh the following materials in parts by weight: 30 parts of octamethylcyclotetrasiloxane, 20 parts of acrylic acid, 15 parts of ethanol, 20 parts of polyethylene oxide Ethylene, 3 parts of xylene and 15 parts of dimethyl phthalate; 2) The above materials were mixed and stirred at a constant temperature of 55°C for 6 hours to obtain a glass coating.
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com