A manufacturing method and technology for seat cushions, which are applied in mattresses, spring mattresses, filled cushions, etc., can solve problems such as difficulty in achieving comfort, and achieve the effects of avoiding bacterial infection, relieving human fatigue, and having good elasticity.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1: A kind of manufacturing method of health care cushion, comprises the following steps successively:
[0020] (1) Raw material preparation: 94.6wt% rubber, 1.2wt% antibacterial agent, 1.2wt% pigment, 3.0wt% vulcanizing agent;
[0021] (2) Mixing: Use a rubber mixer to mix the raw materials in step (1) evenly, and control the mixing time to 30 minutes;
[0022] (3) Vulcanization molding: Put the mixed rubber mixed uniformly in step (2) into the mold for heating and vulcanization to finalize the shape, the temperature is controlled at 180°C, and the time is 4 minutes;
[0023] (4) demoulding.
[0024] The rubber is nitrile rubber or silicon rubber or thermoplastic polyurethane elastomer rubber; the pigment is iron oxide red or iron oxide green or phthalocyanine green G or phthalocyanine blue BGS or carbon black; the vulcanizing agent is bis-pentasulfurization agent or double two four vulcanizing agent or platinum vulcanizing agent.
Embodiment 2
[0025] Embodiment 2: A kind of manufacturing method of health care cushion, comprises the following steps successively:
[0026] (1) Raw material preparation: 95.5wt% of nitrile rubber, 1wt% of antibacterial agent, 1wt% of pigment and 2.5wt% of vulcanizing agent; (2) Mixing: use a rubber mixer to mix the raw materials in step (1) evenly, Control mixing time is 40 minutes;
[0027] (3) Vulcanization molding: put the mixed rubber mixed uniformly in step (2) into the mold, heat and vulcanize and shape it, and control the temperature at 170°C for 3 minutes;
[0028] (4) demoulding.
[0029] The pigment is iron oxide red or iron oxide green or phthalocyanine green G or phthalocyanine blue BGS or carbon black; the vulcanizing agent is double pentasulfurizing agent or double two tetrasulfurizing agent or platinum vulcanizing agent; the antibacterial agent is nano silver.
Embodiment 3
[0030] Embodiment 3: the rubber of 96.4wt%, the antibacterial agent of 0.8wt%, the pigment of 0.8wt%%, the vulcanizing agent of 2.0wt%;
[0031] (2) Mixing: Use a rubber mixer to mix the raw materials in step (1) evenly, and control the mixing time to 45 minutes;
[0032] (3) Vulcanization molding: put the mixed rubber mixed uniformly in step (2) in the mold, heat and vulcanize and shape it, and control the temperature at 175°C for 3.5 minutes;
[0033] (4) demoulding.
[0034] The rubber is nitrile rubber or silicon rubber or thermoplastic polyurethane elastomer rubber; the pigment is iron oxide red or iron oxide green or phthalocyanine green G or phthalocyanine blue BGS or carbon black; the vulcanizing agent is bis-pentasulfurization agent or double two four vulcanizing agent or platinum vulcanizing agent.