Bridge maintenance method
A bridge and curing agent technology, applied in bridges, bridge maintenance, bridge reinforcement, etc., can solve problems affecting the service life of bridges, hidden dangers, aging, etc., and achieve the effect of improving service life, preventing damage, and preventing rapid aging.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0023] The preparation method of the bridge maintenance agent is as follows: stir the modified asphalt and heat it to 180 degrees, add lubricating oil, continue to stir for 30 minutes, cool down to 130 degrees Celsius, and add styrene-butadiene block copolymer, refined carbon Five resins, high-pressure low-density polyethylene and fatty alcohol polyoxyethylene ether, stirred for 60 minutes, cooled to 110°C, added n-butanol and cyclohexanone, stirred for 30 minutes, cooled to 50°C, added UV absorber and glycerin, Stirring for 30 minutes and subpackaging to obtain a curing solution; stirring and mixing the stone chips, glass slag powder and rubber powder before subpackaging to obtain an additive mixture. When spraying the bridge curing agent, first block the bridge and clean the bridge deck; spray 200g / m on the entire bridge deck 2 of the curing solution, sprinkled on it with 50g / m 2 Add the mixture to form the first curing layer; then spray 150g / m on the first curing layer 2 ...
Embodiment 1
[0026] A maintenance method for a bridge, said method comprising the steps of:
[0027] Step 1. Establish a bridge information database to count and record the location, size, type, construction time and repairs since construction of all bridges in the city;
[0028] Step 2. Check the bridge at least every half month, including whether the subsidence of the bridge deck, temperature cracks, fatigue cracks and looseness occur, and report the results in an accurate and timely manner and update the recorded bridge information;
[0029] Step 3, the place where the crack occurs is bonded with an adhesive, and the adhesive is composed of the following components in the following parts by weight: emulsified asphalt: talcum powder: antifreeze: methylene chloride: dichloroprene ene: mustard oil = 80:10:2:20:30:40;
[0030]Step 4. In the absence of abnormal conditions, spray the bridge maintenance agent every six months. The bridge maintenance agent includes a maintenance solution and a...
Embodiment 2
[0035] A maintenance method for a bridge, said method comprising the steps of:
[0036] Step 1. Establish a bridge information database to count and record the location, size, type, construction time and repairs since construction of all bridges in the city;
[0037] Step 2. Check the bridge at least every half month, including whether the subsidence of the bridge deck, temperature cracks, fatigue cracks and looseness occur, and report the results in an accurate and timely manner and update the recorded bridge information;
[0038] Step 3, the place where the crack occurs is bonded with an adhesive, and the adhesive is composed of the following components in the following parts by weight: emulsified asphalt: talcum powder: antifreeze: methylene chloride: dichloroprene ene: mustard oil = 80:10:2:20:30:40;
[0039] Step 4. In the absence of abnormal conditions, spray a bridge maintenance agent every six months. The bridge maintenance agent includes a maintenance solution and an...
PUM
| Property | Measurement | Unit |
|---|---|---|
| Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com