Aqueous crackle coating

A cracked paint, water-based technology, applied in the field of paint, can solve the problems of poor paint film feel, poor adhesion, environmental and human health hazards, etc., and achieve the effect of good adhesion, excellent resistance, and broad market prospects

Active Publication Date: 2013-08-07
SKSHU PAINT
View PDF4 Cites 19 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, it itself contains solvents, so it must be diluted with a large amount of organic solvents containing benzene, alcohols, esters or ketones, which is very harmful to environmental pollution and human health, and is a flammable and explosive product, which is harmful to production. fire hazards in construction sites
In addition, oil-based cracked paint has poor adhesion after forming beautiful lines, and the paint film has poor hand feeling and is not delicate. It must be covered with a top coat to ensure the durability of the lines.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

example 1

[0065] Example 1, a kind of preparation technology of water-based crack coating is as follows:

[0066] (1) The weight percentage of each component of the primer is as follows:

[0067] Water dispersible cationic epoxy resin 80%

[0068] Water-based fungicide 0.15%

[0069] Water-based defoamer 0.05%

[0070] Water-based color paste 5.0%

[0071] Water 14.8%

[0072] First, put the water-dispersible cationic epoxy resin into the dispersion tank; secondly, add the water-based bactericide dosage, water-based defoamer, water-based color paste and the remaining water 600r / min into the dispersion tank slowly while stirring, and stir for 20 minutes. Can.

[0073] (2) The weight percentage of each component of the topcoat is as follows:

[0074] Water (first part) 39%

[0075] Water-based multifunctional additive 0.2%

[0076] Aqueous dispersant 0.3%

[0077] Aqueous wetting agent 0.15%

[0078] Water-based defoamer 0.2%

[0079] Water-Based Matte Powder 13%

[0080] Tita...

example 2

[0087] Example 2, a kind of preparation technology of water-based crack coating is as follows:

[0088] (1), the percentage by weight of each component of primer is identical with example 1.

[0089] (2) The weight percentage of each component of the topcoat is as follows:

[0090] Water (first part) 32%

[0091] Water-based multifunctional additive 0.2%

[0092] Aqueous dispersant 0.3%

[0093] Aqueous wetting agent 0.15%

[0094] Water-based defoamer 0.2%

[0095] Water-Based Matte Powder 10%

[0096] Titanium dioxide 15%

[0097] Room temperature self-crosslinking acrylic emulsion 35%

[0098] Dipropylene glycol butyl ether 1.1%

[0099] Water-based fungicide 0.15%

[0100] Water-based color paste 3.0%

[0101] Water (second part) 2.9%

[0102] First, put water (the first part), water-based multifunctional additives, water-based dispersant, water-based wetting agent, and water-based defoamer into the dispersion tank, and stir at 600r / min for 10 minutes; secondly,...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The present invention relates to an aqueous crackle coating characterized by comprising: a primer and a topcoat, wherein the primer comprises the following components, by weight: water-dispersible cationic epoxy resin 40-95%, an aqueous sterilizing agent 0.1-0.4%, an aqueous antifoaming agent 0.03-0.2%, a water-based color paste 0-10%, and the balance water; and the topcoat comprises the following components, by weight: water 30-45%, an aqueous multifunctional additive 0.05-0.3%, an aqueous dispersant 0.2-0.4%, an aqueous wetting agent 0.1-0.2%, the aqueous antifoaming agent 0.05-0. 4%, an aqueous matte powder 8-15%, titanium dioxide 0-20%, a room temperature self-crosslinking acrylic emulsion 27-45%, dipropylene glycol butyl ether 0.6-1.5%, an aqueous sterilizing agent 0.1 -0.4%, a water-based color paste 0-10%, and the balance water. The aqueous crackle coating of the present invention is environmentally friendly, safe and no hidden trouble, and has a good adhesion to various substrates, and a good flexibility; the film feels fine and smooth, and by adopting the aqueous crackle coating of the invention, one can choose whether a finish coat is needed or not according to the actual situation.

Description

technical field [0001] The invention relates to a water-based crack paint, which is a paint developed in comparison with the existing oil-based crack paint. Background technique [0002] At present, oil-based crack paint is widely used in home decoration and middle-to-high-end handicraft decoration with its beautiful pattern and elegant decoration. However, it itself contains solvents, so it should be diluted with a large amount of organic solvents containing benzene, alcohols, esters or ketones, which is very harmful to environmental pollution and human health, and is a flammable and explosive product, which is harmful to production There are fire hazards in the construction site. In addition, the oil-based cracked paint has poor adhesion after forming beautiful lines, and the paint film feels poor and not delicate. It must be covered with a top coat to ensure the durability of the lines. Contents of the invention [0003] The purpose of the present invention is to prov...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D163/00C09D133/00C09D7/12C09D5/28
Inventor 洪杰何玲玲
Owner SKSHU PAINT
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products