[0021] A preparation method of spray-free water mark is prepared by the following steps:
[0022] (a) Make a corresponding number of screen printing plates according to the pattern to be printed and the type of color, and each printing plate realizes the attachment of the pattern to be printed by film exposure, and corresponds to the corresponding color and the pattern of the color area;
[0023] (b) Place the water-soluble bottom paper in the printing workshop for 2 hours before printing. The temperature of the printing workshop is controlled at 23°C and the relative humidity is controlled at 50% to make the bottom paper adaptable to the environmental conditions in the printing workshop Of water absorption or release;
[0024] (c) The pattern to be printed on the printing plate is printed on the bottom paper with a layer of transparent resin primer through a printing machine to play the role of subsequent stretching and adhesion of ink;
[0025] (d) According to the color type of the...
Embodiment 2
[0030] A method for preparing spray-free water mark is prepared by the following steps:
[0031] (a) Make a corresponding number of screen printing plates according to the pattern to be printed and the type of color, and each printing plate realizes the attachment of the pattern to be printed by film exposure, and corresponds to the corresponding color and pattern of the color;
[0032] (b) Place the water-soluble base paper in the printing workshop for 4 hours before printing. The temperature of the printing workshop is controlled at 25°C and the relative humidity is controlled at 60% to make the base paper adaptable to the environmental conditions in the printing workshop Of water absorption or release;
[0033] (c) The pattern to be printed on the printing plate is sprayed on the bottom paper with a layer of transparent resin primer through the printing machine to play the role of subsequent stretching and ink adhesion;
[0034] (d) According to the color type of the pattern to be ...
Embodiment 3
[0039] A preparation method of spray-free water mark is prepared by the following steps:
[0040] (a) Make a corresponding number of screen printing plates according to the pattern to be printed and the type of color, and each printing plate realizes the attachment of the pattern to be printed by film exposure, and corresponds to the corresponding color and pattern of the color;
[0041] (b) Place the water-soluble base paper in the printing workshop for 6 hours before printing. The temperature of the printing workshop is controlled at 24°C and the relative humidity is controlled at 55% to make the base paper adaptable to the environmental conditions in the printing workshop Of water absorption or release;
[0042] (c) The pattern to be printed on the printing plate is sprayed on the bottom paper with a layer of transparent resin primer through the printing machine to play the role of subsequent stretching and ink adhesion;
[0043] (d) According to the color type of the pattern to be...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com