[0019] Steam sterilize the tea stems at 100°C for 30 minutes and dry them in the air; pulverize them with a pulverizer and sieve them to a particle size of 400 mesh; Dissolve the powder; then add 5 parts of dispersant (DA-01), 1 part of wetting agent (T283), 1 part of defoamer, stir for 10 minutes, after all the added raw materials are fully dissolved; slowly add titanium dioxide (rutile type ) 75 parts, heavy calcium (400-800 mesh) 200 parts, light calcium (400-800 mesh) 200 parts, talcum powder (400-800 mesh) 50 parts, kaolin 100 parts, aluminum silicate 30 parts, with 1500r / Stir for 50 minutes, mix the powder evenly, and grind it with a nano-sand mill. The grinding temperature should not be higher than 55°C until the fineness is ≤70μm; Add 200 parts of the slurry, and stir slowly at 200r / min for 20min; add 1 part of film-forming aid, 1 part of defoamer, and 1 part of preservative (NordesC15), then adjust the pH to 8 with ammonia water, and stir at 200r / min Stir for 30 min...
Embodiment 2
[0021] Steam sterilize the tea stems at 120°C for 20 minutes and dry them in the air; pulverize them with a grinder and sieve them to a particle size of 300 mesh; powder dissolved; then add 7 parts of dispersant (DA-01), 2 parts of wetting agent (T283), 3 parts of defoamer, stir for 15 minutes, after all the added raw materials are fully dissolved; slowly add titanium dioxide (rutile type ) 70 parts, heavy calcium (400-800 mesh) 190 parts, light calcium (400-800 mesh) 210 parts, talcum powder (400-800 mesh) 40 parts, kaolin 90 parts, aluminum silicate 25 parts, at 2000r / min and stir for 30min, after mixing the powder evenly, grind it with a sand mill, the grinding temperature should not be higher than 55℃, until the fineness is ≤70μm; Add the slurry in one portion and stir slowly at 300r / min for 25min; add 2 parts of coalescent, 3 parts of defoamer, and 2 parts of preservative (NordesC15), then adjust the pH to 9 with ammonia water, and stir at 300r / min 30min; Finally, after...
Embodiment 3
[0023] Steam sterilize the tea stems at 110°C for 25 minutes, and dry them in the air; pulverize them with a pulverizer, and sieve them to a particle size of 500 mesh; Dissolve the powder; then add dispersant (DA-0110 parts, wetting agent (T283) 3 parts, defoamer 4 parts, stir for 20 minutes, after all the added raw materials are fully dissolved; slowly add titanium dioxide (rutile type) 80 210 parts of heavy calcium (400-800 mesh), 190 parts of light calcium (400-800 mesh), 60 parts of talcum powder (400-800 mesh), 110 parts of kaolin, 35 parts of aluminum silicate, stirring at 1700r / min After 40 minutes, mix the powder evenly, grind it with a sand mill, and the grinding temperature should not be higher than 55°C until the fineness is ≤70μm; put the above homogenate into the mixing tank, and then add 190 parts of styrene-acrylic emulsion (HBC-03) Slurry, stir slowly at 300r / min for 25min; add 2 parts of film-forming aid, 2 parts of defoamer, and 1 part of preservative (Nordes...
PUM
| Property | Measurement | Unit |
|---|---|---|
| particle size (mesh) | aaaaa | aaaaa |
| particle size (mesh) | aaaaa | aaaaa |
| particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More