A technology of slow-release granules and phosphoric acid, which is applied in application, animal feed, additional food elements, etc., can solve the problems of short action time, poor use effect, and small action area, so as to promote healthy growth, wide action area, and slow-release long-lasting effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] According to the contents provided by the present invention, the inventor has obtained the finished product 1 of sustained-release granular phosphoric acid for feed, the proportioning of raw materials by weight percentage and the preparation process are as follows:
[0027] Raw material ratio: 50% phosphoric acid, 30% carrier silicon dioxide, 5% HPMC, 15% monoglyceride.
[0028] According to the above raw material ratio, the preparation method of the slow-release granular phosphoric acid finished product 1 for feeding is as follows:
[0029] Step 1: Material Preparation
[0030] Weigh the following raw materials according to the formula ratio: phosphoric acid, silicon dioxide, HPMC, monoglyceride;
[0031] Step 2: Dissolving, mixing and adsorption
[0032] A) the weighed HPMC is dissolved in water;
[0033] b) Atomizing and spraying the weighed phosphoric acid into a mixer to mix and absorb with powdery silicon dioxide, and obtain phosphoric acid powder after sieving...
Embodiment 2
[0037] According to the contents provided by the present invention, the inventor has obtained the finished product 2 of sustained-release granular phosphoric acid for feed, the raw material proportioning and preparation process by weight percentage are as follows:
[0038] Raw material ratio: 60% phosphoric acid, 25% carrier silicon dioxide, 2% HPMC, 13% monoglyceride.
[0039] According to the above raw material ratio, the preparation method of the slow-release granular phosphoric acid finished product 2 for feeding is as follows:
[0040] Step 1: Material Preparation
[0041] Weigh the following raw materials according to the formula ratio: phosphoric acid, silicon dioxide, HPMC, monoglyceride;
[0042] Step 2: Dissolving, mixing and adsorption
[0043] A) the weighed HPMC is dissolved in water;
[0044]b) Atomizing and spraying the weighed phosphoric acid into a mixer to mix and absorb with powdery silicon dioxide, and obtain phosphoric acid powder after sieving, and set...
Embodiment 3
[0048] According to the content provided by the present invention, the inventor has obtained the finished product 3 of sustained-release granular phosphoric acid for feed, the raw material proportioning and preparation process by weight percentage are as follows:
[0049] Raw material ratio: 40% phosphoric acid, 40% carrier silicon dioxide, 2.5% HPMC, 2.5% CMC, 5% monoglyceride, 10% diglyceride.
[0050] According to the above raw material ratio, the preparation method of the slow-release granular phosphoric acid finished product 3 for feeding is as follows:
[0051] Step 1: Material Preparation
[0052] Weigh the following raw materials according to the formula ratio: phosphoric acid, silicon dioxide, HPMC and CMC, monoglyceride and diglyceride;
[0053] Step 2: Dissolving, mixing and adsorption
[0054] A) the weighed HPMC and CMC are dissolved in water;
[0055] b) Atomizing and spraying the weighed phosphoric acid into a mixer to mix and absorb with powdery silicon diox...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology