Resource utilization method of waste toner in printer and copying machine
A technology for copiers and printers, which is applied in the field of resource utilization of waste toner, can solve the problems of difficult recycling of waste toner, cumbersome recycling process, and high recycling cost, and achieve high recycling rate, simple process, and low recycling cost Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] Concentrate the waste toner of printers and copiers, use a 20-mesh standard sieve to sieve and remove impurities from the waste toner, add 5wt% Mg(OH) 2 and 0.8wt% engine oil, mixed evenly, activated, the activation time is 2h, and dried at 65°C to prepare the filling reinforcing agent. The above-mentioned filling and reinforcing agent was added to the raw material EPDM rubber, and EPDM rubber was prepared according to the traditional rubber preparation process. The commonly used filling and reinforcing agent carbon black was used as a comparison. Its properties are shown in Table 1.
[0019] Table 1
[0020]
Embodiment 2
[0022] Concentrate the waste toner of printers and copiers, use a 20-mesh standard sieve to sieve and remove impurities from the waste toner, add 2.5wt% Mg(OH) 2 , 1.5wt% Ca(OH) 2 and 0.5wt% engine oil, mix evenly, activate, the activation time is 2.5h, and dry at 105°C to prepare the filling reinforcing agent. Add the above-mentioned filling and reinforcing agent to the raw material styrene-butadiene rubber, and prepare styrene-butadiene rubber according to the traditional rubber preparation process. The commonly used filling and reinforcing agent carbon black is used as a comparison, and its properties are shown in Table 2.
[0023] Table 2
[0024]
Embodiment 3
[0026] Concentrate the waste toner of printers and copiers, use a 20-mesh standard sieve to sieve and remove impurities from the waste toner, add 1.0wt% Mg(OH) 2 , 1.0wt% Ca(OH) 2 , 1.0wt%Al(OH) 3 and 0.2wt% engine oil, mixed evenly, activated for 3 hours, and dried at 85°C to obtain a filling reinforcing agent. The above-mentioned filling and reinforcing agent was added to the raw material nitrile rubber, and the nitrile rubber was prepared according to the traditional rubber preparation process. The commonly used filling and reinforcing agent carbon black was used as a comparison, and its properties are shown in Table 3.
[0027] table 3
[0028]
[0029] In summary, as a filling and reinforcing agent for rubber, the treated waste carbon powder is equivalent to pure carbon black, which can effectively improve the tensile strength and hardness of rubber products, reduce its wear, and can be used as a source Wide range of low cost rubber filled reinforcements.
PUM
Login to View More Abstract
Description
Claims