Washable paper product environment-friendly printing ink and preparation method thereof
A printing ink, washable technology, used in inks, household appliances, applications, etc., can solve the problems of easy decolorization, printing patterns are not washable, etc., to achieve the effect of good water resistance, non-decolorization price, and avoidance of waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment
[0024] In the following examples, the raw materials of each component are commercially available, and the unit is (kg) unless otherwise specified.
[0025] Element Dosage rosin 15.0 preservative 4.5 ethanol 6.0 pigment 32.5 Ethylene glycol tetrabutyrate 1.0 tap water 1.0 Non-silicon polyether mineral oil 1.0 Modified silicone wax copolymer 0.0 water 40.0
[0026] The preparation process is as follows:
[0027] (1) Base material preparation, first put the modified rosin into the reaction kettle according to the formula amount, turn on the mixer and put in water, preservatives, and ethylene glycol tetrabutyric acid in sequence;
[0028] (2) Raise the temperature in the reactor to 70°C and stir for 2 hours, and control the heating temperature at 78°C;
[0029] (3) After the stirring is completed, cool to room temperature, add tap water, modified silicone wax copolymer, and ethanol in proportion, stir for anothe...
Embodiment 4
[0044] Element Dosage rosin 20.0 preservative 6.5 ethanol 13.0 pigment 19.5 Ethylene glycol tetrabutyrate 1.0 tap water 0.0 Non-silicon polyether mineral oil 1.0 Modified silicone wax copolymer 0.0 water 39.0
[0045] The preparation process is as follows:
[0046] (1) Base material preparation, first put the modified rosin into the reaction kettle according to the formula amount, turn on the mixer and put in water, preservatives, and ethylene glycol tetrabutyric acid in sequence;
[0047] (2) Raise the temperature in the reactor to 70°C and stir for 2 hours, and control the heating temperature at 78°C;
[0048] (3) After the stirring is completed, cool to room temperature, add tap water, modified silicone wax copolymer, and ethanol in proportion, stir for another 15 minutes, and store it in a packaging barrel for later use;
[0049] (4) For preparation, add pigments to the base material according to the pro...