A fire-proof filling material for isolation and fire protection in underground caving areas of coal mines
A technology of filling material and caving area, which is applied in the field of high-causing areas of underground roadways, isolated fire-proof filling materials in underground caving areas of coal mines, and isolation of fire-proof filling materials in roof-caving areas of stopes. Poor quality, high cost of filling materials, etc., to achieve the effect of high bonding strength, fast setting and light weight
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] The invention provides a coal mine underground caving zone isolation fireproof filling material, which is composed of the following materials by weight percentage: 18-22% of hydrophobic expanded vitrified microbeads, 42.5% of ordinary Portland cement, 23-28% of water, 41% of water ~46%, JW-I naphthalene series retarding superplasticizer 0.14~0.18%, foaming agent aluminum powder 2.2~2.6%, quick-setting agent sulfoaluminate cement 3.2~3.6%, dispersible latex powder 0.35~ 0.55%, 0.20-0.27% of hydroxypropyl methylcellulose and 4.5-5.5% of red mud are mixed together to form.
Embodiment 2
[0015] The invention provides a coal mine underground caving zone isolation fireproof filling material, which is composed of the following materials in weight percentage: 20% of hydrophobic expanded vitrified microbeads, 42.5-25% of ordinary Portland cement, 43% of water, JW- I naphthalene series retarding superplasticizer 0.16%, foaming agent aluminum powder 2.3%, quick-setting agent sulfoaluminate cement 3.4%, dispersible latex powder 0.5%, hydroxypropyl methylcellulose 0.25% and red mud 5.39% mixed together to make up.
Embodiment 3
[0017] The invention provides a coal mine underground caving zone isolation fireproof filling material, which is composed of the following materials by weight percentage: 16% of hydrophobic expanded vitrified microbeads, 42.5% of ordinary Portland cement, 41% of water, JW- I Naphthalene series retarding superplasticizer 0.1%, foaming agent aluminum powder 3.0%, quick-setting agent sulfoaluminate cement 4.0%, dispersible latex powder 0.3%, hydroxypropyl methylcellulose 0.1% and red Mud 5.5% mixed together to make up.
PUM
| Property | Measurement | Unit |
|---|---|---|
| compressive strength | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
| time | aaaaa | aaaaa |