[0016] Weigh the barks of pine, mulberry, and persimmon trees according to the mass percentage 1:1, put each bark into a pulverizer after mixing, and then pass through a 140-mesh sieve. The resulting material after sieving is a bark mixture, and the bark The mixture and sodium carbonate are mixed according to the mass ratio of 1:3, and water is added to prepare a solution with a mass concentration of 30%, which is allowed to stand for 10 hours, and then put into a beaker to heat the solution and keep the temperature at 70-75°C for cooking. The substance obtained after drying is set aside, then the substance is mixed with sodium humate at a mass ratio of 1:2, and water is added to prepare a solution with a mass concentration of 35%. Cooking is carried out, and the obtained after the water is completely evaporated is the sphalerite inhibitor.
Embodiment 2
[0018] Take eucalyptus, pomegranate bark by mass percentage 1:1.2, put into pulverizer after each bark is mixed and pulverize, pass 150 mesh sieves then, the gained material after sieving is bark mixture, bark mixture and vulcanization The mass ratio of sodium is 1:4, add water to prepare a solution with a mass concentration of 35%, let it stand for 11 hours, then put it into a beaker to heat the solution and keep the temperature at 70-75°C for cooking, and obtain it after the water is evaporated to dryness The substance is set aside, then the substance is mixed with sodium humate at a mass ratio of 1:2.5, and water is added to prepare a solution with a mass concentration of 30%, and the resulting solution is stirred for 3 hours to make the mixture even, and then cooked at 65-75°C. After the water is completely evaporated, the inhibitor of sphalerite is obtained.
Embodiment 3
[0020] Take mulberry tree, persimmon tree, pomegranate bark by mass percentage 1:1.5, put into pulverizer after each bark is mixed and pulverize, then pass 170 mesh sieves, the obtained material after sieving is bark mixture, bark The mixture and sodium carbonate are mixed according to the mass ratio of 1:3, and water is added to prepare a solution with a mass concentration of 30%, which is allowed to stand for 10 hours, and then put into a beaker to heat the solution and keep the temperature at 70-75°C for cooking. The substance obtained after drying is set aside, then the substance is mixed with sodium humate at a mass ratio of 1:2, and water is added to prepare a solution with a mass concentration of 35%. Cooking is carried out, and the obtained after the water is completely evaporated is the sphalerite inhibitor.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com