Embodiment 1
[0037] ① Raw material preparation: See Table 1 for the weight percentage of each raw material of the light-diffusing coating, wherein the particle size of PMMA particles is 1-2 μm, the particle size of PBMA is 7 μm, and the particle size of PS is 3 μm;
[0038] ②Light diffusion coating configuration: first, cyclohexanone, butyl acetate, ethyl acetate, polyether modified polydimethylsiloxane, leveling agent, dispersant, poly-n-butyl methacrylate (PBMA), Add polystyrene (PS) and PMMA particles into the disperser to disperse for 20-30min at a stirring speed of 1600rpm / min, then add acrylic resin to disperse for 15-20min at a stirring speed of 800rpm / min, and finally add aliphatic polyisocyanate to disperse for 15-20min. The stirring speed is 800rpm / min, and the light-diffusing coating is obtained;
[0039] ③Front coating: Apply the light-diffusing coating prepared in step ② evenly on the PET carrier layer (the haze of the PET carrier layer is below 2.5%, and the light transmittan...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com