specific Embodiment approach 1
[0034] Embodiment 1: A preparation method of a mesoporous apatite nano-drug carrier with reduction responsiveness and cell-targeting to liver cancer cells according to this embodiment is carried out according to the following steps:
[0035] 1. Preparation of the template agent: Dissolve the template agent F127 and calcium pantothenate monohydrate in deionized water, and stir at a stirring speed of 250r / min to 400r / min until a clear emulsion is obtained to obtain a F127-calcium pantothenate mixed solution. Promptly obtain templating agent;
[0036] The mass ratio of template agent F127 described in step one to calcium pantothenate monohydrate is 1:(4~8); the mass ratio of template agent F127 described in step one to deionized water is 1:(30~100 );
[0037] 2. Preparation of mesoporous hydroxyapatite nanoparticles: K 2 HPO 4 ·3H 2 O is dissolved in deionized water to give K 2 HPO 4 solution, followed by NH 3 ·H 2 O Mediation K 2 HPO 4 The pH value of the solution is a...
specific Embodiment approach 2
[0055] Embodiment 2: The difference between this embodiment and Embodiment 1 is that the mass ratio of template agent F127 and calcium pantothenate monohydrate described in step 1 is 2.68:17.67. Other steps and parameters are the same as those in the first embodiment.
specific Embodiment approach 3
[0056] Embodiment 3: The difference between this embodiment and Embodiment 1 or 2 is that the mass ratio of template agent F127 to deionized water in step 1 is 2.68:100. Other steps and parameters are the same as those in Embodiment 1 or 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com