A kind of coating agent and its preparation method and application
A film coating agent and formula technology, applied in the field of film coating agent and its preparation, can solve the problems of loss of integrity, dry cracking, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0020] The preparation method of film coating agent of the present invention comprises pretreatment, preparation steps, specifically comprises:
[0021] A. Pre-processing:
[0022] Method 1: Weigh the raw materials konjac glucomannan and chitosan in the formula ratio, add konjac glucomannan into distilled water with a solid-liquid volume ratio of 99 times, keep stirring in a water bath at 40-50°C for 10-30 minutes and set aside Add chitosan to the acid solution with a solid-to-liquid volume ratio of 49 times, and keep stirring in a water bath at 40-50°C for 20-40 minutes for later use;
[0023] Method 2: Weigh the raw materials konjac glucomannan, chitosan and soybean protein isolate in the formula ratio, add konjac glucomannan into distilled water with a solid-liquid volume ratio of 99 times, and keep stirring in a water bath at 40~50°C 10-30min for standby; chitosan was added to the acid solution with a solid-liquid volume ratio of 49 times, and kept stirring in a water bat...
Embodiment 1
[0044] Weigh 1g of konjac glucomannan and 2g of chitosan as raw materials, add konjac glucomannan into distilled water with a solid-to-liquid volume ratio of 1:99, and keep stirring in a water bath at 40-45°C for 30 minutes for later use; chitosan is added to In the acetic acid solution with a solid-to-liquid volume ratio of 2:98, keep stirring in a water bath at 45-50°C for 20 minutes for later use; mix each raw material solution and add 8g of plasticizer, and keep stirring in a water bath at 65-70°C for 20 minutes to obtain the target product.
Embodiment 2
[0046] Weigh 1g of konjac glucomannan and 2g of chitosan as raw materials, add konjac glucomannan into distilled water with a solid-to-liquid volume ratio of 1:99, keep stirring in a water bath at 45-50°C for 10 minutes for later use; add chitosan to In the hydrochloric acid solution with a solid-to-liquid volume ratio of 2:98, keep stirring in a water bath at 40-45°C for 40 minutes for later use; mix each raw material solution and add 8g of plasticizer, and keep stirring in a water bath at 60-70°C for 20-40 minutes to obtain the target product .