Primer-topcoat weather-resistant exterior wall paint and preparation method therefor
An exterior wall paint and weather-resistant technology, applied in the direction of coating, etc., can solve the problems of high cost and complicated painting process, and achieve the effect of short processing time, uniform and delicate stirring, and simple and easy-to-operate preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0042] A weather-resistant exterior wall paint with bottom surface integrated, characterized in that it includes component A, component B, component C and component D, and the component A includes the following components by weight: 175 parts of water, 3.5 parts of cellulose 1 part of bentonite, 2 parts of nitrite, 4 parts of sodium salt dispersant, 3 parts of ammonium salt dispersant, 1 part of wetting agent,
[0043] 2 parts of preservatives, 2 parts of defoamers, and 0.5 parts of regulators; the component B includes the following ingredients in parts by weight: 220 parts of titanium dioxide, 100 parts of coarse powder ground calcium carbonate, and 75 parts of fine powder ground calcium carbonate ; The component C includes the following components by weight: 35 parts of alcohol fat twelve film-forming aids, 1 part of bactericide, and 25 parts of water; the component D includes the following components by weight: 350 parts of acrylic acid emulsion, 2.5 parts of defoamer, 1 pa...
Embodiment 2
[0046] The preparation method of the bottom-surface-integrated weather-resistant exterior wall paint described in Embodiment 1 comprises the following steps:
[0047] Put the components in the component A into the container one by one and stir at a speed of 800-900 rpm for 20-30 minutes to disperse and dissolve into a slurry mixture i;
[0048] Put the component B into the step Stir the dissolved mixture i at a speed of 1200 rpm for 30 minutes until a mixture ii with a fineness of not more than 50um is formed;
[0049] Put the component C into the step Stir in the formed mixture ii for 5 minutes at a speed of 800 to 900 rpm, disperse and dissolve into mixture iii;
[0050] Put the component D into the step The formed mixture iii was stirred at a speed of 600-700 rpm for 10 minutes, dispersed and dissolved until the viscosity was 100-105 ku for exterior wall paint.
[0051] Preferably, the steps , , and The pH value in the water is controlled at 7.5 to 8....