A technology of covering silk and nylon, which is applied in the field of synthetic fibers, can solve the problems of poor product quality, performance uniformity and stability, complex processing procedures, and long process flow, etc., and achieve high dyeing uniformity and added value, simple procedures, The effect of short process flow
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0016] This embodiment provides a method for producing nylon 6POY / spandex stretched false-twisted covered yarn with a specification of 2040 / 34 in one step. For the process flow, refer to the attached figure 1 . The production process conditions are as follows:
[0017] Nylon 6 POY is fed into the heating box device through the first roller and twist stopper for heating, then it is fed into the false twister through the cooling plate for stretching and false twisting to obtain nylon 6 textured yarn (DTY), and then through the tension self-checking device, the nylon 6DTY The stretched spandex is fed into the doubling device at different speeds, the second roller is sent to the vortex type air pressure coating device for coating processing, and then the coated yarn is oiled and coiled by the auxiliary roller and oiling device. The winding device is used for winding forming, and the nylon 6POY / spandex stretched false-twisted covered yarn is produced in one step.
[0018] The mai...
Embodiment 2
[0025] This embodiment provides a method for producing nylon 6POY / spandex stretched false-twisted covered yarn with a specification of 3040 / 24 in one step. For the process flow, see the attached figure 1 .
[0026] The production process and conditions are as follows: Nylon 6 POY is fed into the heating box device through the first roller and twist stopper for heating, and then fed into the false twister through the cooling plate for stretching and false twisting to obtain nylon 6 textured yarn (DTY). Inspection device, input nylon 6DTY and spandex stretched to a certain number of times at different speeds at the same time into the doubling device, the second roller to the vortex air pressure coating device for coating processing, and then pass through the auxiliary roller and oiling device for coating Coated yarn oiling and winding device for winding forming, one-step method to produce nylon 6POY / spandex stretched false twist covered yarn. Its main process parameters are: he...
Embodiment 3
[0028] This embodiment provides a method for producing nylon 6POY / spandex stretched false-twisted covered yarn with a specification of 4070 / 44 in one step. For the process flow, refer to the attached figure 1 .
[0029] The production process conditions are as follows: Nylon 6 POY is input into the heating box device through the first roller and the twist stopper to be heated, and then fed into the false twister through the cooling plate for stretching and false twisting to obtain nylon 6 textured yarn (DTY), and then pass the tension self-test The device, the nylon 6DTY and the spandex stretched to a certain number of times are simultaneously fed into the doubling device at different speeds, the second roller is sent to the vortex air pressure coating device for coating, and then the coated yarn is coated by the auxiliary roller and the oiling device. The oiling and winding device is used for winding and forming, and the nylon 6POY / spandex stretched false-twisted covered yarn...
PUM
| Property | Measurement | Unit |
|---|---|---|
| elongation at break | aaaaa | aaaaa |
| elongation at break | aaaaa | aaaaa |
| elongation at break | aaaaa | aaaaa |