Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Waterproof anti-crack environment-friendly coating and preparation method thereof

An environmentally friendly coating and attapulgite technology, applied in the field of coatings, can solve problems that affect the appearance and use, coating cracks, and unsatisfactory waterproof performance, so as to achieve the effect of improving waterproof performance and crack resistance, and good application prospects

Inactive Publication Date: 2015-12-16
SUZHOU FAST INFORMATION TECH CO LTD
View PDF3 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The waterproof performance of the existing environmentally friendly coatings is not ideal. At the same time, after the repeated process of rainwater washing and sun exposure, as well as when the temperature is too low, it is easy to cause cracks or even fall off of the coating, which affects the appearance and use.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] A preparation method for a waterproof and anti-cracking environmental protection coating, comprising the steps of:

[0018] S1: Mix 35 parts of attapulgite, 12 parts of sericite and 10 parts of titanium dioxide into a grinder and grind to 250-300 mesh to obtain substance A;

[0019] S2: add substance A, 20 parts of styrene-acrylic emulsion and 11 parts of polyethylene glycol in the step S1 together into the stirring device, and stir and react at a temperature of 60° C. for 20 minutes to obtain substance B;

[0020] S3: 8 parts of betulin, 12 parts of hydroxypropyl methylcellulose and 7 parts of glycerol phosphate were sequentially added to the substance B in step S2 under continuous stirring, and the reaction was performed at a temperature of 80°C for 15 minutes; then Then add 2 parts of silver oxide, 3 parts of zinc sulfate and 2 parts of carbohydrazide, and continue the secondary reaction for 40 minutes; after cooling and drying, the waterproof and anti-cracking envir...

Embodiment 2

[0029] A preparation method for a waterproof and anti-cracking environmental protection coating, comprising the steps of:

[0030] S1: Mix 55 parts of attapulgite, 16 parts of sericite and 17 parts of titanium dioxide into a grinder to grind only 300-400 meshes to obtain substance A;

[0031] S2: Add substance A, 30 parts of styrene-acrylic emulsion and 18 parts of polyethylene glycol in the step S1 together into a stirring device, and stir and react at a temperature of 80° C. for 40 minutes to obtain substance B;

[0032] S3: Add 15 parts of betulin, 16 parts of hydroxypropyl methylcellulose and 13 parts of glycerol phosphate to the substance B in step S2 under constant stirring, and react at a temperature of 100°C for 20 minutes; then Then add 8 parts of silver oxide, 7 parts of zinc sulfate and 7 parts of carbohydrazide, and continue the secondary reaction for 60 minutes; after cooling and drying, the waterproof and crack-resistant environmental protection coating can be ob...

Embodiment 3

[0041] A preparation method for a waterproof and anti-cracking environmental protection coating, comprising the steps of:

[0042] S1: Mix 42 parts of attapulgite, 14 parts of sericite and 12 parts of titanium dioxide into a grinder and grind to 250-300 mesh to obtain substance A;

[0043] S2: add substance A, 22 parts of styrene-acrylic emulsion and 12 parts of polyethylene glycol in the step S1 together into a stirring device, and stir and react at a temperature of 70° C. for 30 minutes to obtain substance B;

[0044] S3: Add 10 parts of betulin, 13 parts of hydroxypropyl methylcellulose and 8 parts of glycerol phosphate to the substance B in step S2 under constant stirring, and react at a temperature of 90°C for 15 minutes; then Then add 4 parts of silver oxide, 5 parts of zinc sulfate and 4 parts of carbohydrazide, and continue the secondary reaction for 50 minutes; after cooling and drying, the waterproof and anti-cracking environmental protection coating can be obtained....

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
elongationaaaaaaaaaa
elongationaaaaaaaaaa
elongationaaaaaaaaaa
Login to View More

Abstract

The invention discloses a preparation method of waterproof anti-crack environment-friendly coating. The preparation method comprises the following steps: mixing 35 to 55 parts of attapulgite, 12 to 16 parts of sericite, and 10 to 17 parts of titanium dioxide to obtain a mixture I, putting the mixture I into a grinding machine for grinding, so as to obtain a substance A; adding the substance A, 20 to 30 parts of a styrene-acrylic emulsion and 11 to 18 parts of polyethylene glycol into a stirring device, and carrying out stirring at 60 to 80 DEG C for reaction, so as to obtain a substance B; adding 8 to 15 parts of betulin, 12 to 16 parts of hydroxypropyl methyl cellulose, and 7 to 13 parts of phosphoglyceride into the substance B in sequence under the condition that stirring is carried out continuously, and carrying out a primary reaction at 80 to 100 DEG C; adding 2 to 8 parts of silver oxide, 3 to 7 parts of zinc sulfate, and 2 to 7 parts of carbohydrazide, and carrying out a secondary reaction for 40 to 60 minutes; carrying out cooling and drying to obtain the waterproof anti-crack environment-friendly coating. The waterproof anti-crack environment-friendly coating prepared according to the preparation method not only has application properties of common coating, but also is environment-friendly, generates no pollution to human bodies and the ambient environment, and is excellent in water resistance and anti-crack property, and wide in application prospect.

Description

technical field [0001] The invention belongs to the field of coatings, and relates to a waterproof and anti-cracking environmental protection coating and a preparation method thereof. Background technique [0002] Coatings are mixtures of polymer substances and other ingredients that can be applied to the surface of a substrate to form firm adhesion. At present, coatings have become my country's five major synthetic materials along with plastics, synthetic rubber, synthetic fibers, and adhesives. The development of the coatings industry is an important symbol of the development level of a country's chemical industry. During the drying and film-forming process of traditional coatings, harmful volatile gases will be released into the air, which seriously threatens human health. Therefore, the research on coatings is increasingly inclined to the direction of environmentally friendly coatings. The waterproof performance of existing environmental protection coatings is not ideal...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): C09D125/14C09D171/02C09D101/28C09D7/12
Inventor 彭孝茹
Owner SUZHOU FAST INFORMATION TECH CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products