Non-bright face unsmooth-wax-feeling treating agent for synthetic leather and preparing method thereof
A synthetic leather, astringent wax feeling technology, applied in the direction of fiber processing, textiles and papermaking, etc., to achieve the effect of increasing production costs, excellent abrasion resistance, and strong astringent wax feeling on the leather surface
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0019] The matte, astringent and waxy feeling treatment agent for synthetic leather consists of the following components: 35 parts by weight of polyurethane, 35 parts by weight of dimethylformamide, 15 parts by weight of dichloroethane, 2 parts by weight of silica matting powder, 4 parts by weight of oleic acid amide, and 1 part by weight of dispersant.
[0020] The preparation method of the above-mentioned matte and astringent waxy feeling treatment agent for synthetic leather is: under normal temperature and pressure, 17.5 parts by weight of polyurethane, 35 parts by weight of dimethylformamide, 15 parts by weight of dichloroethane, 2 parts by weight of Part of silica matting powder, 4 parts by weight of oleic acid amide, 1 part by weight of dispersant mix, stir at least 30 minutes until the mixture is uniformly mixed and grind and filter, add the remaining 17.5 parts by weight of polyurethane in the above mixture obtained , stirred for at least 30 minutes until the mixture ...
Embodiment 2
[0023] The matte, astringent, waxy feeling treatment agent for synthetic leather consists of the following components: 37 parts by weight of polyurethane, 37 parts by weight of dimethylformamide, 16 parts by weight of dichloroethane, 4 parts by weight of silica matting powder, 5 parts by weight of oleic acid amide, and 1 part by weight of dispersant.
[0024] The preparation method of the above-mentioned matte and astringent waxy feeling treatment agent for synthetic leather is: under normal temperature and pressure, 18.5 parts by weight of polyurethane, 37 parts by weight of dimethylformamide, 16 parts by weight of dichloroethane, 4 parts by weight of Part of silica matting powder, 5 parts by weight of oleic acid amide, 1 part by weight of dispersant mix, stir at least 30 minutes until the mixture is uniformly mixed and grind and filter, add the remaining 18.5 parts by weight of polyurethane in the above mixture obtained , stirred for at least 30 minutes until the mixture is ...
Embodiment 3
[0027] The matte, astringent, waxy feeling treatment agent for synthetic leather consists of the following components: 40 parts by weight of polyurethane, 40 parts by weight of dimethylformamide, 17 parts by weight of dichloroethane, 4 parts by weight of silica matting powder, 5 parts by weight of oleic acid amide, and 2 parts by weight of dispersant.
[0028] The preparation method of the above-mentioned matte astringent waxy feeling treatment agent for synthetic leather is: under normal temperature and pressure, 20 weight parts of polyurethane, 40 weight parts of dimethylformamide, 17 weight parts of dichloroethane, 4 weight parts Part of silica matting powder, 5 parts by weight of oleic acid amide, 2 parts by weight of dispersant mix, stir at least 30 minutes until the mixture is evenly mixed and grind and filter, add the remaining 20 parts by weight of polyurethane in the above mixture obtained , stirred for at least 30 minutes until the mixture is evenly mixed, and then g...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com