Durable exterior wall coating material and preparation method thereof

An exterior wall coating, durable technology, applied in the direction of anti-corrosion coatings, coatings, etc., can solve the problems of poor weather resistance, etc., to achieve the effect of long service life, short drying time, high water resistance and alkali resistance

Inactive Publication Date: 2016-04-20
曲少春
View PDF1 Cites 1 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The engineering latex paint of the prior art has the disadvantage of poor weather resistance, so it is necessary to develop a high-quality engineering latex paint that can improve its weather resistance

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Durable exterior wall coating material and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0014] The invention is a durable exterior wall paint, which is made of the following raw materials in parts by weight: 3 parts of 4-methylstyrene, 10 parts of titanium dioxide, 25 parts of white latex, 2.5 parts of sodium hexametaphosphate, deionized water 7.3 parts, 1.5 parts of 2,5,6-trimethyl-4-heptenal, 2.2 parts of dibenzylphenol polyoxyethylene ether, 2.5 parts of nitrocellulose film-forming agent, cis-1,2-dimethylol 1.3 parts of vinyl ethylene and 2.8 parts of dimethyl 1,2-phthalate.

[0015] A preparation method of a durable exterior wall paint, comprising the following steps:

[0016] 1) Weigh according to the formula, add 4-methylstyrene and titanium dioxide into the dispersion tank, add the deionized water of the formula amount, and disperse and stir at 400r / min for 15min;

[0017] 2) Then add the formula amount of white latex and sodium hexametaphosphate, and disperse at a high speed of 800r / min for 15min;

[0018] 3) Then add the 2,5,6-trimethyl-4-heptenal and ...

Embodiment 2

[0022] The invention is a durable exterior wall paint, which is made of the following raw materials in parts by weight: 7 parts of 4-methylstyrene, 15 parts of titanium dioxide, 33 parts of white latex, 4.6 parts of sodium hexametaphosphate, deionized water 8.1 parts, 3.8 parts of 2,5,6-trimethyl-4-heptenal, 6.3 parts of dibenzylphenol polyoxyethylene ether, 26.5 parts of nitrocellulose film-forming agent, cis-1,2-dimethylol 3.2 parts of vinyl ethylene and 6.2 parts of dimethyl 1,2-phthalate.

[0023] A preparation method of a durable exterior wall paint, comprising the following steps:

[0024] 1) Weigh according to the formula, add 4-methylstyrene and titanium dioxide into the dispersion tank, add the deionized water of the formula amount, and disperse and stir at 500r / min for 20min;

[0025] 2) Then add the formula amount of white latex and sodium hexametaphosphate, and disperse at a high speed of 1000r / min for 25min;

[0026] 3) Then add the 2,5,6-trimethyl-4-heptenal an...

Embodiment 3

[0030] The invention is a durable exterior wall paint, which is made of the following raw materials in parts by weight: 6 parts of 4-methylstyrene, 13 parts of titanium dioxide, 27 parts of white latex, 3.5 parts of sodium hexametaphosphate, deionized water 7.7 parts, 2.7 parts of 2,5,6-trimethyl-4-heptenal, 4.2 parts of dibenzylphenol polyoxyethylene ether, 4.8 parts of nitrocellulose film-forming agent, cis-1,2-dimethylol 1.6 parts of vinyl ethylene and 3.7 parts of dimethyl 1,2-phthalate.

[0031] A preparation method of a durable exterior wall paint, comprising the following steps:

[0032] 1) Weigh according to the formula, add 4-methylstyrene and titanium dioxide into the dispersion tank, add the deionized water of the formula amount, and disperse and stir at 450r / min for 18min;

[0033] 2) Then add the formula amount of white latex and sodium hexametaphosphate, and disperse at a high speed of 900r / min for 20min;

[0034] 3) Then add the 2,5,6-trimethyl-4-heptenal and ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a durable exterior wall coating material, which is prepared from the following raw materials in parts by weight: 3 to 7 parts of 4-vinyltoluene, 10 to 15 parts of titanium pigments, 25 to 33 parts of white emulsions, 2.5 to 4.6 parts of sodium hexametaphosphate, 7.3 to 8.1 parts of deionized water, 1.5 to 3.8 parts of 2,5,6-trimethyl-4-heptenal, 2.6 to 6.3 parts of dibenzylphenol polyoxyethylene ether, 2.5 to 6.5 parts of nitric acid fiber film forming agents, 1.3 to 3.2 parts of cis-1,2-dihydroxymethyl ethylene, and 2.8 to 6.2 parts of 1,2-dimethyl phthalate. Compared with an existing product, the durable exterior wall coating material is good in low temperature stability, high in water resistance and alkali resistance, has anti-scrubbing times of 2000 to 2500 times, is long in service life, is not abnormal when a coating is subjected to a temperature fluctuation resistance test for over 5 times, and is short in drying time; a paint film is level, attractive and elegant in appearance.

Description

technical field [0001] The invention relates to a durable exterior wall coating and a preparation method thereof, belonging to the field of architectural coatings. Background technique [0002] Engineering latex paint is latex paint used in engineering, and its ingredients are usually composed of petrochemical raw materials such as vinyl acetate, acrylate, styrene emulsion, titanium dioxide, talcum powder and some additives. The engineering latex paint of the prior art has the disadvantage of poor weather resistance, so it is necessary to develop a high-quality engineering latex paint that can improve its weather resistance. Contents of the invention [0003] Aiming at the deficiencies in the prior art, the technical problem to be solved by the present invention is to provide a durable exterior wall paint and a preparation method thereof, which not only meet the properties of latex paint, but also have excellent weather resistance. [0004] In order to solve the above tec...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09D151/00C09D7/12C09D5/08C08F263/04
CPCC09D151/00C08F263/04C08L2205/03C09D5/08C09D7/61C09D7/63C09D7/65C08L71/02C08L1/18C08K2003/2241C08K3/32C08K5/12C08F212/12
Inventor 曲少春
Owner 曲少春