Drilling fluid with strong inhibition and strong plugging and preparation method thereof
A technique of drilling fluid and inhibition, which is applied in the field of drilling fluid and its preparation, can solve the problems of good anti-slump performance, and achieve the effects of preventing wellbore collapse, good wellbore collapse, and inhibiting hydration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0016] Cationic polyamine is the reaction product of butylenediamine, butylene oxide and epoxychlorobutane. The preparation method is to add butylene oxide dropwise to butylenediamine under the condition of stirring and 100℃, react for 1h, and then The temperature was raised to 140°C, and epichlorobutane was added dropwise under stirring, formic acid was added for 1 hour of reaction, and the reaction was continued for 1 hour to obtain a polyamine inhibitor sample. Control the molar ratio of butanediamine, butylene oxide, epoxychlorobutane and formic acid to 1:4:0.4:0.8, and its kinematic viscosity is 456.4mm 2 / s, cationic degree is 0.906mmol / g. The preparation method of the amino compound is to add 103g of diethylenetriamine and 0.5g of potassium hydroxide under stirring, mix well, heat up to 80°C, and gradually add 232g of propylene oxide (the molar ratio of propylene oxide to diethylenetriamine is 4 : 1), after the dropwise addition, react at 80°C for 8h, cool down to room...
Embodiment 2
[0020] Cationic polyamine is the reaction product of butylenediamine, butylene oxide and epoxychlorobutane. The preparation method is to add butylene oxide dropwise to butylenediamine under the condition of stirring and 100℃, react for 1h, and then The temperature was raised to 140°C, and epichlorobutane was added dropwise with stirring, formic acid was added for 1 hour of reaction, and the reaction was continued for 1 hour to obtain a polyamine inhibitor sample. Control the molar ratio of butanediamine, butylene oxide, epoxychlorobutane and formic acid to 1:4:0.4:0.8, and its kinematic viscosity is 456.4mm 2 / s, cationic degree is 0.906mmol / g. The preparation method of the amino compound is to add 146g of triethylenetetramine and 0.73g of potassium hydroxide under stirring, mix well, heat up to 90°C, and gradually add 116g of propylene oxide (the molar ratio of propylene oxide to diethylenetriamine is 3 : 1), after the dropwise addition, react at 90°C for 10h, cool down to r...
Embodiment 3
[0024] Cationic polyamine is the reaction product of butylenediamine, butylene oxide and epoxychlorobutane. The preparation method is to add butylene oxide dropwise to butylenediamine under the condition of stirring and 100℃, react for 1h, and then The temperature was raised to 140°C, and epichlorobutane was added dropwise with stirring, formic acid was added for 1 hour of reaction, and the reaction was continued for 1 hour to obtain a polyamine inhibitor sample. Control the molar ratio of butanediamine, butylene oxide, epoxychlorobutane and formic acid to 1:4:0.4:0.8, and its kinematic viscosity is 456.4mm 2 / s, cationic degree is 0.906mmol / g. The preparation method of the amino compound is to add 146g of triethylenetetramine and 0.94g of potassium hydroxide under stirring, mix well, heat up to 100°C, and gradually add 116g of propylene oxide (the molar ratio of propylene oxide to diethylenetriamine is 2 : 1), after the dropwise addition, react at 100°C for 9h, cool down to ...