Ceramic pigment pretreatment method
A ceramic pigment and pretreatment technology, applied in the field of ceramic production, can solve the problem of pigment precipitation, etc., and achieve the effects of reducing the generation of air bubbles, avoiding pinholes, and improving the water-locking function.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] A pretreatment method for ceramic pigments, comprising the following steps:
[0016] S1. Mix and stir the CMC macromolecular compound, bentonite, honey and water. The content of each component is calculated in parts by weight: 95 parts of CMC macromolecular compound, 10 parts of bentonite, 2.5 parts of honey, and 5000 parts of water;
[0017] S2. Put the mixed solution obtained in step S1 into a grinding cylinder for grinding for 24 hours to form a translucent liquid;
[0018] S3. Add the translucent liquid prepared in step S2 into the color material, and fully stir to form a spare color material, which is stored for later use, wherein the weight ratio of the translucent liquid to the color material is 5:100.
Embodiment 2
[0020] A pretreatment method for ceramic pigments, comprising the following steps:
[0021] S1. Mix and stir the CMC macromolecular compound, bentonite, honey and water. The content of each component is calculated in parts by weight: 100 parts of CMC macromolecular compound, 5 parts of bentonite, 2 parts of honey, and 4500 parts of water;
[0022] S2. Put the mixed solution obtained in step S1 into a grinding cylinder for grinding for 24 hours to form a translucent liquid;
[0023] S3. Add the translucent liquid prepared in step S2 into the color material, and fully stir to form a spare color material, which is stored for later use, wherein the weight ratio of the translucent liquid to the color material is 5:100.
Embodiment 3
[0025] A pretreatment method for ceramic pigments, comprising the following steps:
[0026] S1. Mix and stir the CMC macromolecular compound, bentonite, honey and water. The content of each component is calculated in parts by weight: 105 parts of CMC macromolecular compound, 7.5 parts of bentonite, 5 parts of honey, and 4000 parts of water;
[0027] S2. Put the mixed solution obtained in step S1 into a grinding cylinder for grinding for 24 hours to form a translucent liquid;
[0028] S3. Add the translucent liquid prepared in step S2 into the color material, and fully stir to form a spare color material, which is stored for later use, wherein the weight ratio of the translucent liquid to the color material is 5:100.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com